Abstract
Tailings containing pyrite generate acid drainage and still contain gold that direct cyanidation fails to recover. The Santa Catalina tailings (Peru), containing 2.4 g/t Au, 62 g/t Ag, and about 60% pyrite, were studied. Although more than 99% of the pyrite was liberated, direct cyanidation extracted only 13–14% of the gold. The tailings were roasted at temperatures between 400 and 800 °C using two particle sizes, and the calcines were cyanidated. Scanning electron microscopy revealed 2 µm gold particles and silver tellurides containing gold in the pyrite of the calcines at 400–500 °C. The pyrite transformed into porous hematite from the edge toward the center, passing through pyrrhotite. Grinding to 95% −38 µm lowered the temperature required for sulfur removal by about 100 °C compared to 60% −75 µm. The optimal condition—600 °C with fine grinding—extracted 52.7% of the gold and 37.7% of the silver. At 800 °C, gold extraction dropped to 25–27%, likely due to the formation of Zn and Cu ferrites. Temperature accounted for 68% of the variation in gold extraction. To scale up the process, it is advisable to first concentrate the pyrite by flotation and to reduce the high cyanide consumption caused by copper.

This publication has 39 references indexed in Scilit: