Hot drawn Fe–6.5wt.%Si wires with good ductility
Authors:
- W. YangWYW. Yang
- H. LiHLH. Li
- K. YangKYK. Yang
- Y.F. LiangYLY.F. Liang
- J. YangJYJ. Yang
- F. YeFYF. Ye
- 1 August 2014
- journal article
- Published by Elsevier in Materials Science and Engineering: B
- Vol. 186, 79-82
Abstract
No abstract availableKeywords
This publication has 13 references indexed in Scilit:
- Effect of annealing temperature on magnetic properties of cold rolled high silicon steel thin sheetJournal of Alloys and Compounds, 2010
- Microstructure and Magnetic Properties of Fe-6.5wt%Si Alloy Obtained by Spray Forming ProcessMaterials Science Forum, 2005
- Ordering and grain growth in nanocrystalline Fe75Si25 alloyActa Materialia, 2005
- Magnetic properties of high silicon iron sheet fabricated by direct powder rollingJournal of Magnetism and Magnetic Materials, 2004
- High-silicon steel produced by hot dipping and diffusion annealingJournal of Applied Physics, 2002
- The influence of an ordering transition on the interdiffusion in Fe-Si alloysActa Metallurgica et Materialia, 1995
- The influence of critical points and structure and microstructural evolution in iron rich FeSi alloysActa Metallurgica et Materialia, 1993
- Mechanical properties of Fe-4.5-6wt.%Si double roller ribbonsMaterials Science and Engineering: A, 1991
- Commercial scale production of Fe-6.5 wt. % Si sheet and its magnetic propertiesJournal of Applied Physics, 1988
- Annealing of silicon-iron ribbons containing around 6.5 wt% siliconIEEE Transactions on Magnetics, 1981