Safety issues of defective lithium-ion batteries: identification and risk evaluation
- 2 June 2020
- journal article
- research article
- Published by Royal Society of Chemistry (RSC) in Journal of Materials Chemistry A
- Vol. 8 (25) , 12472-12484
Abstract
Lithium-ion batteries inevitably suffer minor damage or defects caused by external mechanical abusive loading, e.g., penetration, deformation, and scratch without triggering a hard/major short circuit. The replacement of cells becomes a dilemma if the safety risk of the defective batteries remains unknown. Herein, by introducing a representative defect form, i.e., screw indentation, we demonstrate the safety characteristics of defective batteries. We prove that defective batteries have a significantly increased thermal risk and deteriorated mechanical integrity, but can go undetected due to prompt voltage recovery and insignificant local temperature increase. We discover that the voltage curve within the first few cycles contains sufficient information to identify defective batteries from otherwise good ones and propose methodologies to monitor the cells. Capacity loss and current leakage are two characteristics that can be estimated using the voltage curve. According to the defect size and position, the capacity loss could be 1 to 102 mA h and the leakage current could be 5–50 mA. Results remove the barriers for defective battery safety risk evaluation, enabling identification, monitoring, and early warning of minor damaged batteries.Keywords
This publication has 30 references indexed in Scilit:
- Modeling Nail Penetration Process in Large-Format Li-Ion CellsJournal of the Electrochemical Society, 2014
- An electrochemical modeling of lithium-ion battery nail penetrationJournal of Power Sources, 2014
- Thermal runaway caused fire and explosion of lithium ion batteryJournal of Power Sources, 2012
- Electrical Energy Storage for the Grid: A Battery of ChoicesScience, 2011
- Lithium batteries: Status, prospects and futureJournal of Power Sources, 2010
- Building better batteriesNature, 2008
- A three-dimensional thermal abuse model for lithium-ion cellsJournal of Power Sources, 2007
- Thermal Model of Cylindrical and Prismatic Lithium-Ion CellsJournal of the Electrochemical Society, 2001
- Simulation and Optimization of the Dual Lithium Ion Insertion CellJournal of the Electrochemical Society, 1994
- Modeling of Galvanostatic Charge and Discharge of the Lithium/Polymer/Insertion CellJournal of the Electrochemical Society, 1993