Effects of Scandium on Corrosion Resistance and Mechanical Properties of Cellular Al-Based Foams

Authors:

Abstract
Cellular Al-0.24wt.%Sc and Al-0.41wt.%Sc foams with a porosity ranging from 37 to 86% were successfully fabricated via the melt-foaming method with the calcium particles as the thickening agent and titanium hydride as blowing agent. The corrosion rate increased with the increasing of porosity for the cellular Al-0.24wt.%Sc, Al-0.41wt.%Sc and Al foams. Large size Al3Sc precipitates can accelerate the corrosion of the Al foams. However, T6-treatments could improve the corrosion resistance significantly. With T6-treatments, 0.24 wt.%Sc addition to Al foams exhibited unconspicuous decrease in the corrosion resistance but much improved strength.

This publication has 13 references indexed in Scilit: