Two-body wear of monolithic, veneered and glazed zirconia and their corresponding enamel antagonists
- 30 January 2012
- journal article
- Published by Medical Journals Sweden AB in Acta Odontologica Scandinavica
- Vol. 71 (1) , 102-112
Abstract
Objective. This study tested whether the two-body wear of monolithic zirconia and their corresponding enamel antagonists was higher compared to monolithic alloy and veneered zirconia. Materials and methods. Cylindrical specimens (N = 36, n = 6) were prepared out of (A) veneered zirconia (VZ), (B) glazed zirconia using a glaze ceramic (GZC), (C) glazed zirconia using a glaze spray (GZS), (D) manually polished monolithic zirconia (MAZ), (E) mechanically polished monolithic zirconia (MEZ) and (F) monolithic base alloy (control group, MA). Wear tests were performed in a chewing simulator (49 N, 1.7 Hz, 5°C/50°C) with enamel antagonists. The wear analysis was performed using a 3D profilometer before and after 120,000, 240,000, 640,000 and 1,200,000 masticatory cycles. SEM images were used for evaluating wear qualitatively. The longitudinal results were analysed using linear mixed models (α = 0.05). Results. Materials (p < 0.001) and number of masticatory cycles (p < 0.001) had a significant effect on the wear level. The least enamel antagonist wear was observed for MAZ and MEZ (27.3 ± 15.2, 28 ± 11.1 μm, respectively). GZC (118 ± 30.9 μm) showed the highest wear of enamel antagonists. The highest wear rate in the material was observed in GZS (91.3 ± 38.6 μm). While in the groups of MA, VZ, GZC and GZS 50% of the specimens developed cracks in enamel, it was 100% in MAZ and MEZ groups. Conclusion. Polished monolithic zirconia showed lower wear rate on enamel antagonists as well as within the material itself but developed higher rates of enamel cracks.Keywords
This publication has 28 references indexed in Scilit:
- The effect of low temperature aging on the mechanical property & phase stability of Y-TZP ceramicsThe Journal of Advanced Prosthodontics, 2009
- Evaluation of a High Fracture Toughness Composite Ceramic for Dental ApplicationsJournal of Prosthodontics, 2008
- Wear of ceramic and antagonist—A systematic evaluation of influencing factors in vitroDental Materials, 2008
- Compatibility of machined Ce-TZP/Al2O3 nanocomposite and a veneering ceramicDental Materials, 2007
- The efficacy of posterior three-unit zirconium-oxide–based ceramic fixed partial dental prostheses: A prospective clinical pilot studyThe Journal of Prosthetic Dentistry, 2006
- All‐ceramic fixed partial dentures designed according to the DC‐Zirkon® technique. A 2‐year clinical studyJournal of Oral Rehabilitation, 2005
- A critical comparison of methods for the determination of the aging sensitivity in biomedical grade yttria‐stabilized zirconiaJournal of Biomedical Materials Research Part B: Applied Biomaterials, 2004
- Critical effect of cubic phase on aging in 3 mol% yttria-stabilized zirconia ceramics for hip replacement prosthesisBiomaterials, 2004
- Y-TZP ceramics for artificial joint replacementsBiomaterials, 1998
- Crystal Structures of Zirconia Phases and their Inter-RelationKey Engineering Materials, 1998