Shear Bond Strengths of Composite Resin Bonded to MIH-Affected Hard Tissues with Different Adhesives and Pre-Treatments
Open Access
- 20 August 2025
- journal article
- research article
- Published by MDPI AG in Dentistry Journal
- Vol. 13 (8) , 377
Abstract
Background: Reduced bond strengths in hypmineralised enamel have been reported with increased restorative failures. This study aimed to investigate the shear bond strengths of resin composite to hypomineralised enamel and dentin bonded with two different adhesive systems and pre-treatments. Methods: Thirty-six freshly extracted first permanent molars with MIH and 17 sound third molars were used for shear bond strength tests in enamel and dentin. Specimens of control groups were bonded to resin composite using ScotchbondTM Universal Plus and AdperTM Scotchbond 1XT. MIH-affected enamel specimens of six test groups were pre-treated with various chemical agents, such as 35% phosphoric acid, 5% NaOCl, resin infiltration with ICON®, or a combination of these agents prior to bonding with composite resin using ScotchbondTM Universal Plus. Bonded specimens were subsequently sheared at a crosshead speed of 1.0 mm/min, after which their fracture modes were recorded. The mean bond strengths of all groups were compared using a one-way analysis of variance test (ANOVA) and a Bonferroni–Holm analysis was performed for pairwise comparison between the groups. The association between modes of failure was examined with Pearson’s chi-square test. Results: Mean shear bond strength values were highest for sound dentin specimens (Group SD 2) bonded with ScotchbondTM Universal Plus (23.76 ± 7.68 MPa). Sound enamel specimens (Group SE 2) exhibited significantly higher mean bond strength values than MIH-enamel specimens (Group HE 2) when bonded with ScotchbondTM Universal Plus (19.68 ± 6.25 vs. 11.53 ± 3.29 MPa, p < 0.001). Oxidative pre-treatment followed by resin infiltration significantly improved bond strengths to hypomineralised enamel (Group HE 6) (17.84 ± 2.98 MPa, p < 0.05). Bond strengths to sound and hypomineralised enamel and dentin did not differ significantly for both adhesives. Conclusions: Within the limitations of an in vitro study, oxidative pre-treatment in combination with resin infiltration seems to be beneficial when planning adhesive restorations with composite in hypomineralised enamel. Both ScotchbondTM Universal Plus and AdperTM Scotchbond 1XT can be used for bonding of resin composite to MIH-affected enamel and dentin.Keywords
This publication has 51 references indexed in Scilit:
- Epidemiological trends in enamel hypomineralisation and molar-incisor hypomineralisation: a systematic review and meta-analysisClinical Oral Investigations, 2025
- Best clinical practice guidance for clinicians dealing with children presenting with molar-incisor-hypomineralisation (MIH): an updated European Academy of Paediatric Dentistry policy documentEuropean Archives of Paediatric Dentistry, 2021
- Molar-incisor hypomineralisation: an updated view for aetiology 20 years laterEuropean Archives of Paediatric Dentistry, 2021
- An update of the aetiological factors involved in molar incisor hypomineralisation (MIH): a systematic review and meta-analysisEuropean Archives of Paediatric Dentistry, 2021
- Can molar incisor hypomineralization cause dental fear and anxiety or influence the oral health-related quality of life in children and adolescents?—a systematic reviewEuropean Archives of Paediatric Dentistry, 2021
- Distribution and morphology of enamel hypomineralisation defects in second primary molarsEuropean Archives of Paediatric Dentistry, 2020
- Universal dental adhesives: Current status, laboratory testing, and clinical performanceJournal of Biomedical Materials Research Part B: Applied Biomaterials, 2019
- Hypomineralised second primary molars: prevalence, defect characteristics and possible association with Molar Incisor Hypomineralisation in Indian childrenEuropean Archives of Paediatric Dentistry, 2015
- Best Clinical Practice Guidance for clinicians dealing with children presenting with Molar-Incisor-Hypomineralisation (MIH)European Archives of Paediatric Dentistry, 2010
- Retention of fissure sealants using two different methods of application in teeth with hypomineralised molars (MIH): A 4 year clinical studyEuropean Archives of Paediatric Dentistry, 2009