Fracture Resistance of Ceramic Veneers with Different Preparation Designs
Authors:
- Burçin AkoğluBABurçin Akoğlu
- BurçinBUBurçin
- Deniz GemalmazDGDeniz Gemalmaz
- 1 June 2011
- journal article
- Published by Wiley in Journal of Prosthodontics
- Vol. 20 (5) , 380-384
Abstract
The purpose of this study was to examine the fracture load of ceramic veneers with different preparation designs. Seventy-five extracted, intact, human maxillary central incisors were prepared according to five preparation designs (P) (n: 15) as follows: (1) P2e: 2-mm incisal reduction, preparation entirely in enamel; (2) P4e: 4-mm incisal reduction, preparation entirely in enamel; (3) P2d: 2-mm incisal reduction, preparation entirely in dentin; (4) P4d: 4-mm incisal reduction, preparation entirely in dentin; and (6) Pc: Unrestored, intact teeth as control. All preparations had a butt joint incisal finish line, rounded internal line angles, and cervical finish lines 1 mm above the cementoenamel junction. Ceramic veneers were fabricated with IPS Empress (Ivoclar Vivadent AG, Schaan, Liechtenstein) and cemented with Syntac Classic Adhesive system and Variolink II (Ivoclar) resin cement. Veneers were loaded until fracture at a 90° angle to the lingual surface of the test tooth following the thermocycling process (5° to 55°, 3500 times). Statistical analyses were performed using analysis of variance (ANOVA) and Tukey's Multiple Range Test. The mean fracture loads (SD) were (in N) as follows: (1) P2e: 262 (63); (2) P4e: 189 (40); (3) P2d: 239 (53); (4) P4d: 162 (36); and (5) Pc: 277 (66). The amount of incisal reduction exhibited a significant influence on fracture resistance regardless of the preparation depth (p < 0.05). Ceramic veneers with preparation designs entirely on dentin with 4-mm incisal reduction yielded lower fracture loads than those prepared with 2-mm incisal reduction. Veneers with 2-mm incisal reduction exhibited fracture resistance similar to that of intact teeth for preparation designs supplied on both enamel and dentin.Keywords
This publication has 12 references indexed in Scilit:
- Longevity and failure load of ceramic veneers with different preparation designs after exposure to masticatory simulationThe Journal of Prosthetic Dentistry, 2005
- The effect of thermocycling on the strength of porcelain laminate veneer (PLV) materialsDental Materials, 2003
- Tooth structure removal associated with various preparation designs for anterior teethThe Journal of Prosthetic Dentistry, 2002
- Porcelain veneers: a review of the literatureJournal of Dentistry, 2000
- Fracture load and mode of failure of ceramic veneers with different preparationsThe Journal of Prosthetic Dentistry, 2000
- An in vitro assessment of tooth preparation for porcelain veneer restorationsJournal of Dentistry, 1995
- The use of adhesively retained all-porcelain veneers during the management of fractured and worn anterior teeth: Part 2. Clinical results after 5 years of follow-upBritish Dental Journal, 1995
- The effect of dentin bonding agents on the microleakage of porcelain veneersDental Materials, 1994
- A comparative assessment of the strengths of porcelain veneers for incisor teeth dependent on their design characteristicsBritish Dental Journal, 1991
- Microleakage patterns of porcelain and castable ceramic laminate veneersThe Journal of Prosthetic Dentistry, 1989