Abstract
Crystalline oxide films are important components in a wide array of electronic and optical devices, and their study and manufacture involve major aspects of current science and technology. A plethora of methods, such as sputtering, chemical vapor deposition, pulsed laser deposition, and sol-gel, are commonly used to deposit these films, and many new techniques are being developed ([1][1]). In each of these methods, however, the deposited film is amorphous. For those applications requiring a crystalline film, an additional high-temperature processing step is required. This high-temperature step can lead to considerable constraints in combining the desirable characteristics of a crystalline oxide film with those of thermally unstable substrates and other device components. High-temperature processing also adds considerable costs to manufacturing. We describe a simple method that provides a general means for both low-temperature deposition and crystallization of oxide films. To demonstrate the generality of the method, we describe here the production of Zn2SiO4, ZrO2, and MnO2 films, which are of interest for applications in displays, electronics, and energy storage, respectively. The present method derives from our report on the preparation of oxide powders by a method of precipitation and hydrothermal dehydration ([2][2]). In this process, a hydroxo precipitate is dehydrated under hydrothermal conditions to yield an anhydrous, crystalline oxide at temperatures as low as 400 K. We have now combined this dehydration and crystallization process with the successive-ionic-layer-adsorption-and-reaction (SILAR) deposition method ([3][3]) to produce fully crystalline oxide films at low temperatures. In the SILAR process, the cation constituent is first adsorbed onto the substrate surface, followed by a rinsing step in water to produce an approximate monolayer of coverage. The substrate is then transferred to a solution containing the anionic constituent, wherein a precipitation reaction occurs at the surface of the substrate; the process is completed with an additional water rinse. This cycle of coating and rinsing is repeated many times under robotic control to achieve a desired film thickness. For the examples given here, substrates were immersed in ∼0.1 M solutions and rinse baths for 10 s each, and 700 cycles were used to develop a film thickness near 250 nm. Dehydration was performed overnight (∼12 hours), although crystallinity in some systems has been observed after a 30-min treatment. Films of Zn2SiO4 were produced on glass and nitrided silicon (Si3N4/Si) substrates by using the SILAR process with Zn2+(aq) and SiO4 4−(aq) as the cationic and anionic constituents, respectively. The SiO4 4−(aq) species undergoes extensive hydrolysis, so the as-deposited film is an amorphous hydrated hydroxide salt. The film was crystallized by heating at 378 K in a sealed 23-ml Teflon-lined Parr reactor containing 0.15 ml of water (pressure ∼ 12 atm). From consideration of the x-ray diffraction patterns in [Fig. 1][4], A and B, the resulting film is a highly crystalline form of Zn2SiO4. For comparison, annealing the amorphous, as-deposited film near the softening point of the glass substrate (temperature = 923 K) does not produce a crystalline product. ![Figure 1][5]![Figure 1][5] Figure 1 ( A ) X-ray diffraction pattern of Zn2SiO4 film on Si3N4/Si. ( B ) Simulated powder x-ray diffraction pattern of Zn2SiO4. ( C ) Electron micrograph of ZrO2 film on Si3N4/Si substrate. Crystalline films of ZrO2 have been deposited on Si3N4/Si substrates. Again, SILAR deposition with the aqueous solutions Zr4+(aq) and OH−(aq) results in an amorphous, hydroxylated film. After hydrothermal dehydration at 473 K, the resulting diffraction pattern reveals the formation of the expected monoclinic form of ZrO2; an electron micrograph of the resulting film is given in [Fig. 1][4]C. Curiously, direct annealing of the amorphous film in air at 923 K results in the production of an oxygen-deficient tetragonal form of ZrO2-δ, whereas under normal conditions, this phase exists only at temperatures above 1273 K ([4][6]). Annealing the monoclinic film at 923 K results in no structural change. MnO2 and Mn2O3 have been deposited on SiO2/Si substrates by using the solutions Mn2+(aq) and OH−/H2O2(aq). The as-deposited material is amorphous. After a hydrothermal anneal at 473 K, the film is crystalline, forming the tetragonal, rutile form of MnO2([5][7]). Annealing the as-deposited film at 773 K results in loss of oxygen and production of the cubic, bixbyite structure of Mn2O3 ([6][8]). These processing methods thus provide facile control of product formation and oxidation states of the Mn cation. A simple and general method has been demonstrated for both low-temperature thin-film deposition and crystallization of refractory oxides. It provides opportunities for development of manufacturing methods, generation of unusual composite materials, and application of high-temperature materials to low-cost substrates, as shown by the deposition of a green-emitting phosphor on a flexible, plastic substrate (fig. S1) ([7][9]). 1. [↵][10]1. M. Ritala 2. et al. , Science 288, 319 (2000). [OpenUrl][11][Abstract/FREE Full Text][12] 2. [↵][13]1. B. L. Clark, 2. D. A. Keszler , Inorg. Chem. 40, 1724 (2001). [OpenUrl][14][CrossRef][15][PubMed][16][Web of Science][17] 3. [↵][18]1. Y. F. Nicolau , Appl. Surf. Sci. 22, 1061 (1985). [OpenUrl][19] 4. [↵][20]1. U. Martin, 2. H. Boysen, 3. F. Frey , Acta Crystallogr. Sect. B 49, 403 (1993). [OpenUrl][21][CrossRef][22][Web of Science][23] 5. [↵][24]1. W. H. Baur , Acta Crystallogr. Sect. B 32, 2200 (1976). [OpenUrl][25][CrossRef][26][GeoRef][27][Web of Science][28] 6. [↵][29]1. S. Geller , Acta Crystallogr. Sect. B 27, 821 (1971). [OpenUrl][30][CrossRef][31][Web of Science][32] 7. [↵][33]See supplementary information available...Keywords
This publication has 6 references indexed in Scilit:
- Hydrothermal Dehydration of Precipitates: Convenient Synthesis Method for SolidsInorganic Chemistry, 2001
- Atomic Layer Deposition of Oxide Thin Films with Metal Alkoxides as Oxygen SourcesScience, 2000
- Neutron powder investigation of tetragonal and cubic stabilized zirconia, TZP and CSZ, at temperatures up to 1400 KActa crystallographica Section B, Structural science, crystal engineering and materials, 1993
- Solution deposition of thin solid compound films by a successive ionic-layer adsorption and reaction processApplications of Surface Science, 1985
- Rutile-type compounds. V. Refinement of MnO2 and MgF2Acta Crystallographica Section B: Structural Science, Crystal Engineering and Materials, 1976
- Structure of α-Mn2O3, (Mn0.983Fe0.017)2O3 and (Mn0.37Fe0.63)2O3 and relation to magnetic orderingActa Crystallographica Section B: Structural Science, Crystal Engineering and Materials, 1971