Scaling to Sub-1 nm Equivalent Oxide Thickness with Hafnium Oxide Deposited by Atomic Layer Deposition

Authors:

Abstract
The implementation of HfO2HfO2 gate dielectrics in sub- 45nm45nm devices requires optimization of nanometer-thin HfO2HfO2 layers, deposited, e.g., by atomic layer deposition (ALD). In this work, we optimize ALD conditions such as precursor pulse time and deposition temperature for HfO2HfO2 layers with physical thicknesses below 2nm2nm . Additionally, we investigate intermediate treatments in the ALD reaction cycle, such as exposure to gas-phase moisture or remote plasma at low temperature and thermal anneals. Such intermediate treatments affect both growth-per-cycle (GPC) and Cl-impurity content of the HfO2HfO2 layers. The analysis of the process modifications allows a better understanding of the reaction mechanisms. H2OH2O pulse times of 10s10s must be applied to achieve saturation in GPC and Cl content. Using saturated H2OH2O pulses decreases the gate leakage current in the sub- 1nm1nm equivalent oxide thickness (EOT) range. The GPC is enhanced from ∼1.8Hf∕nm2∼1.8Hf∕nm2 for conventional ALD to 4Hf∕nm24Hf∕nm2 for intermediate plasma treatments at low temperature. Intermediate anneals reduce the Cl content by about two orders of magnitude. Sufficient hydroxylation of the HfO2HfO2 surface is one important factor controlling electrical properties in the sub- 1nm1nm EOT range. The reduction of the Cl content does not systematically improve the electrical properties.

This publication has 25 references indexed in Scilit: