Effect of fibre length and chemical modifications on the tensile properties of intimately mixed short sisal/glass hybrid fibre reinforced low density polyethylene composites
Authors:
- 2 August 2004
- journal article
- research article
- Published by Wiley in Polymer International
- Vol. 53 (11) , 1624-1638
Abstract
Hybrid composites prepared by the incorporation of two or more different types of fibres into a single polymer matrix deserve much attention. This method of hybridisation of composites offers a profitable procedure for the fabrication of products while the resulting materials are noted for their high specific strength, modulus and thermal stability. The influence of the relative composition of short sisal/glass fibres, their length and distribution on the tensile properties of short sisal/glass intimately mixed polyethylene composites (SGRP) was examined. Different compositions of sisal and glass such as 70/30, 50/50 and 30/70 have been prepared with varying fibre lengths in the range of 1–10 mm. Emphasis has also been given to the variation of fibre–matrix adhesion with several fibre chemical modifications. Chemical surface modifications such as alkali, acetic anhydride, stearic acid, permanganate, maleic anhydride, silane and peroxides given to the fibres and matrix were found to be successful in improving the interfacial adhesion and compatibility between the fibre and matrix. The nature and extent of chemical modifications were analysed by infrared spectroscopy while improvement in fibre–matrix adhesion was checked by studying the fractography of composite samples using a scanning electron microscope. Assessment of water retention values has been found to be a successful tool to characterize the surface of the stearic acid modified fibres. It was found that the extent of improvement in tensile properties of SGRP varied with respect to the nature of chemical modifications between fibre and matrix. Improved mechanical anchoring and physical and chemical bonding between fibre and polyethylene matrix are supposed to be the reasons for superior tensile strength and Young's modulus in treated composites. Several secondary reasons such as high degree of fibre dispersion and reduced hydrophilicity in chemically modified fibres also are believed to play a role. Among the various chemical modifications, the best tensile strength and modulus was exhibited by the SGRP with benzoyl peroxide treated fibres. This is attributed to the peroxide‐initiated grafting of polyethylene on to the fibres. Copyright © 2004 Society of Chemical IndustryKeywords
This publication has 32 references indexed in Scilit:
- Studies on mechanical performance of biofibre/glass reinforced polyester hybrid compositesComposites Science and Technology, 2003
- Effect of hybridisation on crushing behaviour of carbon/glass fibre/epoxy circular–cylindrical shellsJournal of Materials Processing Technology, 2003
- Electromechanical behavior of hybrid carbon/glass fiber composites with tension and bendingJournal of Applied Polymer Science, 2002
- Sisal fibre and its composites: a review of recent developmentsComposites Science and Technology, 2000
- The effect of chemical treatment on the properties of hemp, sisal, jute and kapok for composite reinforcementDie Angewandte Makromolekulare Chemie, 1999
- The effect of chemical composition of interphase on dispersion of cellulose fibers in polymers. I. PVC‐coated cellulose in polystyreneJournal of Applied Polymer Science, 1993
- Performance of treated hybrid fiber reinforced‐thermoplastic composites under extreme conditions. IV. Use of glass fiber and sawdust as hybrid fiberJournal of Applied Polymer Science, 1991
- Effect of Fiber Treatment on the Mechanical Properties of Hybrid Fiber Reinforced Polystyrene Composites: III. Use of Mica and Sawdust as Hybrid FiberJournal of Reinforced Plastics and Composites, 1991
- Hybrid composites based on polyethylene and carbon fibres Part 2: influence of composition and adhesion level of polyethylene fibres on mechanical propertiesComposites, 1990
- Impact performance of sisal-polyester compositesJournal of Materials Science Letters, 1988