In this paper, we introduced nanocomposite materials as a debonding layer (DBL) in the fabrication of flexible displays. These materials provided flexible substrate with good debonding capability even after 450 o C low‐temperature poly‐silicon (LTPS) process. The effect of temperature on debonding force of flexible substrate was investigated. Besides, some characteristics of thin‐film transistors (TFT) were also studied.