Impacts of glass composition, pH, and temperature on glass forward dissolution rate
Open Access
- 6 August 2018
- journal article
- research article
- Published by Springer Nature in npj Materials Degradation
- Vol. 2 (1) , 22
Abstract
Nuclear waste glasses dissolve at the forward dissolution rate (rf) in very dilute aqueous solutions, which can isolate the impact of the glass composition from solution feedback and alteration product effects. While it has long been known that pH and temperature (T) strongly impact rf, the impacts of glass composition have remained uncertain. In this work, rf data from 19 nuclear waste glasses were used with the aim of identifying the effect of glass composition on rf. The rf values were modeled as: rf = k010–ηpHexp(−Ea/RT), with k0, η, Ea, and R, respectively, being the intrinsic rate constant, pH coefficient, apparent activation energy, and gas constant. However, no predictive correlation could be established between the individual model parameters (log[k0], η, and Ea) and glass composition for the glasses considered in this study, an outcome that was attributed to the strong positive correlation between the log[k0] and Ea parameters. Therefore, a model was fitted directly to the combined rf from all 19 glasses. This approach showed that 90% of the variation in rf data could be accounted for solely by T and pH effects. Therefore, any composition effects must be relatively small. After normalizing for differences in pH and T, the only notable differences in rf between the glasses were found to correlate with variations in the fraction of glass forming tetrahedra contributed by tetrahedral boron, f([4]B), with an abrupt threshold at a high value of f([4]B) (~0.22), where higher rf are predicted with no discernable composition effects below the threshold.Keywords
This publication has 41 references indexed in Scilit:
- An international initiative on long-term behavior of high-level nuclear waste glassMaterials Today, 2013
- Monte Carlo simulations of the dissolution of borosilicate and aluminoborosilicate glasses in dilute aqueous solutionsGeochimica et Cosmochimica Acta, 2011
- Nuclear Waste Vitrification in the United States: Recent Developments and Future OptionsInternational Journal of Applied Glass Science, 2010
- SON68 nuclear glass dissolution kinetics: Current state of knowledge and basis of the new GRAAL modelJournal of Nuclear Materials, 2008
- An experimental study of the dissolution rates of simulated aluminoborosilicate waste glasses as a function of pH and temperature under dilute conditionsApplied Geochemistry, 2008
- The effect of composition on the leaching of three nuclear waste glasses: R7T7, AVM and VRZJournal of Nuclear Materials, 2005
- Compositional Effects on the Long-Term Durability of Nuclear Waste Glasses: A Statistical ApproachMRS Proceedings, 2004
- Measurement of kinetic rate law parameters on a Na-Ca-Al borosilicate glass for low-activity wasteJournal of Nuclear Materials, 1997
- A General Rate Equation for Nuclear Waste Glass CorrosionMRS Proceedings, 1984
- Thermodynamic and kinetic constraints on reaction rates among minerals and aqueous solutions; I, Theoretical considerationsAmerican Journal of Science, 1982