Ferroelectricity in Mn-implanted CdTe

Authors:

Abstract
CdTe:Mn was prepared by implantation of CdTe with 200 keV Mn ions with a dose of 5×1016 cm−2, which produced an insulating layer in the surface region. Ferroelectric characterization of the implanted sample revealed a clear hysteresis in its polarization–voltage curves. The remnant polarization of CdTe:Mn amounts to 0.64 μC/cm2 at 400 Hz, and it decreases with increasing temperature in a continuous and diffusive manner. Capacitance measurement demonstrated a maximum capacitance at 140 °C, and fitting of the data with Curie–Weiss law shows the occurrence of a second-order-type phase transition. The ferroelectricity is accounted for by the cation size difference in CdTe:Mn.