Interfacial Microstructure and Phase Constitution of the Cu/Al Dissimilar Metals Joint Made by Contact Reactive Brazing
Authors:
- 1 March 2010
- journal article
- Published by Trans Tech Publications, Ltd. in Advanced Materials Research
- Vol. 97-101, 3891-3894
Abstract
Joining Cu to Al has been carried out by vacuum contact reactive brazing without filler metal. Experimental results obtained showed that the eutectic structure and some Cu-Al intermetallic compounds were the main phases of the braze seam. The fracture surface of the joint presented typical brittle fracture for the existence of intermetallic compounds at the interface and the shear strength could reach 65MPa.Keywords
This publication has 5 references indexed in Scilit:
- Microstructure and phase constitution near the interface of Cu/Al vacuum brazing using Al–Si filler metalVacuum, 2008
- Microstructural evolution in the friction stir welded 6061 aluminum alloy (T6-temper condition) to copperJournal of Materials Processing Technology, 2006
- Effects of intermetallic compound on the electrical and mechanical properties of friction welded Cu/Al bimetallic joints during annealingJournal of Alloys and Compounds, 2005
- Formation of Al2Cu and AlCu intermetallics in Al(Cu) alloy matrix composites by reaction sinteringMaterials Science and Engineering: A, 2004
- Transient liquid phase diffusion bonding under a temperature gradient: modelling of the interface morphologyActa Materialia, 2001