Abstract
Determining the concentration of electrically active dopants in III–V core–shell nanowires has long been a challenge due to the difficulty of developing ohmic contact with the nanowire core. In this paper, we have used a noncontact optical method to estimate the electron concentration in Si-doped GaAs:Si/Al0.25Ga0.75As core–shell nanowires. The temperature-dependent photoluminescence (PL) spectra of these GaAs:Si/Al0.25Ga0.75As nanowires indicate that at 15 K, the carrier concentration in the conductive core of the core–shell nanowires can be as high as 1.40 × 1018 cm−3. The band-filling effect was considered to accurately determine the concentrations of carriers in the nanowires using optical methods. The highest electron density is achieved for a nominal Si concentration of 1.89 × 1019 cm−3, and a further increase in Si concentration reduces the effective doping level due to the amphoteric behaviour of Si in GaAs. The dependence of the integrated PL intensity on the laser power at T = 15 K exhibits a typical two-thirds power dependence, indicating the presence of a nonradiative Auger recombination mechanism in the nanowire under high carrier concentration.
Funding Information
  • Bundesministerium für Forschung, Technologie und Raumfahrt (03SF0451)

This publication has 45 references indexed in Scilit: