Mechanisms limiting EOT scaling and gate leakage currents of high-k/metal gate stacks directly on SiGe and a method to enable sub-1nm EOT
Authors:
- J. HuangJHJ. Huang
- P. D. KirschPKP. D. Kirsch
- J. OhJOJ. Oh
- S.H. LeeSLS.H. Lee
- J. PriceJPJ. Price
- P. MajhiPMP. Majhi
- H.R. HarrisHHH.R. Harris
- D. C. GilmerDGD. C. Gilmer
- D. Q. KellyDKD. Q. Kelly
- P. SivasubramaniPSP. Sivasubramani
- G. BersukerGBG. Bersuker
- D. HehDHD. Heh
- 1 June 2008
- conference paper
- Published by Institute of Electrical and Electronics Engineers (IEEE)
- p. 82-83
Abstract
For the first time, we provide mechanistic understanding of high gate leakage current on surface channel SiGe pFET with high-k/metal gate to enable sub 1 nm EOT. The primary mechanism limiting EOT scaling is Ge enhanced Si oxidation resulting in a thick (1.4 nm) SiOx interface layer. A secondary mechanism, Ge doping (ges4%) in high-k, possibly by up diffusion, also results in higher leakage. With this understanding, we optimized high-k nitridation reducing O and Ge diffusion to achieve EOT=0.91 nm directly on SiGe with leakage equivalent to bulk Si. High Ion (1.5times Si), and low subthreshold slope (73 mV/dec) are also achieved. This mechanism enables high mobility channel gate dielectric development directly on SiGe without the need for Si cap, simplifying processing and device design.Keywords
This publication has 2 references indexed in Scilit: