High temperature air oxidation behaviour of “poor man” high manganese‐aluminum steels
Authors:
- 1 July 1982
- journal article
- Published by Wiley in Materials and Corrosion
- Vol. 33 (7) , 386-390
Abstract
The behaviour of austenitic high manganese (19.8%–32.5%)aluminum (7.1%–10.2%) steels in high temperature air has been examined. Tests have been carried out in the 600–900°C temperature range for durations up to 200 h. The steels form a high manganese scale at high oxidation rates; aluminum does not contribute to the formation of this scale. Only a 1.5% silicon bearing steel shows a good oxidation resistance up to 700°C, the oxidation rate being lower because as shown by XPS analyses a silicon‐containing scale is formed. The oxidation resistance of these steels is always lower than that of conventional grades of austenitic stainless steels.Keywords
This publication has 3 references indexed in Scilit:
- High temperature scaling behaviour of ferritic stainless steels alloyed with yttriumSurface Technology, 1978
- Versuche mit chromfreien hitzebeständigen StählenArchiv für das Eisenhüttenwesen, 1948
- Die Eisenecke des Systems Eisen-Mangan-AluminiumArchiv für das Eisenhüttenwesen, 1933