Wear Behavior of Graded Glass/Zirconia Crowns and Their Antagonists
- 11 February 2019
- journal article
- research article
- Published by SAGE Publications in Journal of Dental Research
- Vol. 98 (4) , 437-442
Abstract
Monolithic zirconia crowns have become very popular; their surface finish is considered a key factor for restoration longevity. While polishing has shown excellent results in vivo, the surface glass infiltration of zirconia may offer superior damage resistance and aesthetic advantages by using tooth-colored glasses. Thus, the purpose of this study is to evaluate the efficacy of polishing and glass infiltration on the wear behavior of monolithic zirconia crowns. The wear behavior of intact natural molar teeth was investigated as a reference. Zirconia crowns were divided into 3 groups: PolZ—sintered then polished; PolGZ—polished in the presintered state and then glass infiltrated and sintered; NoPolGZ—as machined, glass infiltrated and sintered. Crowns were adhesively bonded to a dentin-like abutment. Zirconia crowns and molar teeth ( n = 15) were subjected to contact-slide-liftoff cyclic loading (200 N, 1.25 million cycles) with a steatite sphere ( r = 3 mm) as an antagonist in water. Surface and subsurface damages were investigated with optical and scanning electron microscopies. Wear depth and volume loss were determined with micro–computed tomography. PolGZ and NoPolGZ crowns exhibited shallow wear scars, where material loss remained within the glass/zirconia layer with no visible cracks. Meanwhile, PolZ crowns presented no visible wear damage. Volume loss (mm3) in the steatite antagonist was as follows (mean ± SD): PolZ = 0.022 ± 0.007, PolGZ = 0.011 ± 0.004, and NoPolGZ = 0.014 ± 0.006. Molar teeth yielded no measurable wear on the antagonist, while the wear scar on the teeth was greater than that on zirconia crowns, ranging from 0.07 to 0.35 mm3. The combination of polishing and glass infiltration on the occlusal surface of monolithic zirconia crowns yielded reduced wear on both crown and antagonist.Keywords
Funding Information
- National Institute of Dental and Craniofacial Research (R01DE017925)
- National Institute of Dental and Craniofacial Research (R01DE026279)
- National Institute of Dental and Craniofacial Research (R01DE026772)
This publication has 32 references indexed in Scilit:
- Three-body wear potential of dental yttrium-stabilized zirconia ceramic after grinding, polishing, and glazing treatmentsThe Journal of Prosthetic Dentistry, 2014
- Sliding contact fracture of dental ceramics: Principles and validationActa Biomaterialia, 2014
- Overview: Damage resistance of graded ceramic restorative materialsJournal of the European Ceramic Society, 2012
- Chipping Resistance of Graded Zirconia Ceramics for Dental CrownsJournal of Dental Research, 2012
- Sliding Contact Fatigue of Graded Zirconia with External Esthetic GlassJournal of Dental Research, 2011
- Wear performance of substructure ceramics and veneering porcelainsDental Materials, 2011
- Graded Zirconia Glass for Resistance to Veneer FractureJournal of Dental Research, 2010
- Graded Structures for All-ceramic RestorationsJournal of Dental Research, 2010
- Graded structures for damage resistant and aesthetic all-ceramic restorationsDental Materials, 2009
- Optimization of ceramic strength using elastic gradientsActa Materialia, 2009