Redox Behaviors of Ni and Cr with Different Counter Cations in Spinel Cathodes for Li-Ion Batteries

Authors:

Abstract
The electrochemical performances of the spinels Li[Ni0.5M1.5]O4Li[Ni0.5M1.5]O4 , Li[CrM]O4Li[CrM]O4 , and Li[MnM]O4Li[MnM]O4 with M=Mn(IV)M=Mn(IV) vs Ti(IV) as cathodes for Li-ion batteries are compared. With M=Mn(IV)M=Mn(IV) , reversible access to the valence states Ni(IV) to Ni(II) and Cr(IV) to Cr(III) is possible at a voltage V≈4.7V≈4.7 and 4.85 V (vs Li+/LiLi+/Li ), respectively. The solid electrolyte interface (SEI) layer formed with M=Mn(IV)M=Mn(IV) at voltages V4.3VV4.3V are Li-permeable. The disproportionation reaction 3Cr(IV)=2Cr(III)+Cr(VI)3Cr(IV)=2Cr(III)+Cr(VI) contributes to the loss of capacity in Li[CrMn]O4Li[CrMn]O4 . With M=Ti(IV)M=Ti(IV) , reversible charge/discharge curves were not obtained between 3.5 and 4.9 V (vs Li+/LiLi+/Li ). The cathode Fermi energy EFCEFC is lowered by about 0.2 eV on charging from M=Mn(IV)M=Mn(IV) to M=Ti(IV)M=Ti(IV) , but this lowering is not sufficient to cause O2O2 evolution from the spinel on charge with M=Ti(IV)M=Ti(IV) . Whereas Li-permeable SEI layers are formed with M=Mn(IV)M=Mn(IV) , we conclude that the SEI layers formed with M=Ti(IV)M=Ti(IV) are Li-blocking. The SEI layer may be a Li-poor, Ti-rich phase formed at the surface of the cathode particle during charge rather than an SEI layer formed by a reaction with the electrolyte.

This publication has 18 references indexed in Scilit: