Effect of the Depth of Decarburized Layer in SKL15 Tension Clamp on Fatigue Strength
Open Access
- 23 April 2021
- journal article
- research article
- Published by MDPI AG in Applied Sciences
- Vol. 11 (9) , 3841
Abstract
The surface of a quenched and tempered spring steel may have a decarburized layer from which the carbon component has been reduced. The fatigue strength of the decarburized layer is low compared to the base metal, which can easily develop fatigue cracks. Recently, fatigue failure was reported in the tension clamp (SKL 15) of the DFF-300 rail fastening system during use on one urban transit route in South Korea. As a result of measuring the depth of the decarburized layer of the SKL 15 tension clamp where the fatigue failure occurred, a decarburized layer thinner than the manufacturer’s maximum allowable decarburized layer was found in one of the eight tension clamps. To check the depth of the decarburized layer where the fatigue crack may have initiated, the decarburized layer was assumed to be the initial crack, and fatigue crack initiation was assessed based on the linear elastic fracture mechanics. The manufacturer’s maximum allowable decarburized layer depth of 0.2 mm may result in fatigue cracks.Keywords
Funding Information
- Incheon National University (2016-2216)
This publication has 3 references indexed in Scilit:
- Failure Analysis of Fatigue Cracking in the Tension Clamp of a Rail Fastening SystemInternational Journal of Steel Structures, 2019
- Fracture mechanics and notch sensitivityFatigue & Fracture of Engineering Materials & Structures, 2003
- The Stress Analysis of Cracks Handbook, Third Edition2000