Experimental and Chitosan-Infused Adhesive with Dentin Pretreated with Femtosecond Laser, Methylene Blue-Activated Low-Level Laser, and Phosphoric Acid
Author:
- 17 October 2024
- journal article
- research article
- Published by SAGE Publications in Photobiomodulation, Photomedicine, and Laser Surgery
- Vol. 42 (10) , 634-642
Abstract
Aim: To prepare experimental adhesive (EA) with 1% and without chitosan nanoparticles on dentin conditioned with a conventional technique phosphoric acid (PA) compared with two different contemporary techniques: photodynamic therapy (PDT) and femtosecond laser (FSL). Method: The methodology consisted of synthesis of EA and 1% chitosan-modified adhesive (CMA). Scanning electron microscopy, dentin adhesive interface assessment, energy-dispersive spectroscopy, shear bond strength (SBS), degree of conversion (DC), and bond failure were assessed. Teeth were selected, disinfected, and mounted in acrylic up to the cementoenamel junction. Occlusal enamel was removed and teeth were randomly allocated into groups and conditioned. These included Group 1: samples treated with PA; Group 2: specimens conditioned with methylene blue photosensitizer (MBP) activated by PDT; and Group 3: samples conditioned with FSL. Following different conditioning regimes, specimens were bonded using 1% CMA and EA. The composite buildup was followed by SBS testing and a bond failure assessment. DC was assessed for both EA and CMA. Analysis of variance and Tukey’s post hoc test were used to compare the mean and standard deviation of SBS and DC in different experimental groups, with a significance level of p < 0.05. Results: Dentin pretreated with etch and rinse demonstrated the highest bond strength with 1% CMA. Dentin conditioned with MBP activated by PDT and bonded to EA showed the lowest bond scores. Overall SBS values of 1% CMA were better than EA irrespective of the conditioning regime of dentin. The DC was higher in EA adhesive. This was followed by DC in 1% CMA. DC in EA was found to be comparable with 1% CMA. Conclusions: PA remains the gold standard for dentin conditioning. The incorporation of 1% chitosan in adhesive improves SBS and results in no change in DC. The use of FSL in dentin conditioning can be used as an alternative approach as it results in SBS within acceptable limits. The study was approved by the ethical board of King Saud University.Keywords
This publication has 48 references indexed in Scilit:
- Chitosan: A review of sources and preparation methodsInternational Journal of Biological Macromolecules, 2021
- Recent Advances in Adhesive Bonding: The Role of Biomolecules, Nanocompounds, and Bonding Strategies in Enhancing Resin Bonding to Dental SubstratesCurrent Oral Health Reports, 2017
- Bond strengths of brackets bonded to enamel surfaces conditioned with femtosecond and Er:YAG laser systemsLasers in Medical Science, 2016
- Photodynamic therapy in dentistry: a literature reviewClinical Oral Investigations, 2012
- Apatite crystal protection against acid-attack beneath resin–dentin interface with four adhesives: TEM and crystallography evidenceDental Materials, 2012
- In vitro comparison of mechanical properties and degree of cure of bulk fill compositesClinical Oral Investigations, 2012
- Durability of bonds and clinical success of adhesive restorationsDental Materials, 2012
- Influence of femtosecond laser treatment on shear bond strength of composite resin bonding to human dentin under simulated pulpal pressureJournal of Biomedical Materials Research Part B: Applied Biomaterials, 2011
- Relationship of solvent to the photopolymerization process, properties, and structure in model dentin adhesivesJournal of Biomedical Materials Research Part A, 2006
- Effect of blood contamination on shear bond strength of brackets bonded with conventional and self-etching primersAmerican Journal of Orthodontics and Dentofacial Orthopedics, 2004