Passive and Active Oxidation of Hot–Pressed Silicon Nitride Materials with Two Magnesia Contents
Author:
- 1 July 1982
- journal article
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 65 (7) , c111-c113
Abstract
Hot‐pressed Si 3 N 4 materials containing 1 and 5 wt% MgO were oxidized for 1000 h at 1000°, 1100°, and 1200°C in helium at 0.4 to 0.8 Pa total oxidants. Transition from passive to active oxidation occurred between 1000° and 1100° C, in agreement with published theoretical calculations for pure Si 3 N 4 . The amounts of both passive and active oxidation were greater for the material containing 5 wt% MgO. Specimen surfaces were porous and oxide–free under active oxidation conditions but contained porous oxide at transition.Keywords
This publication has 9 references indexed in Scilit:
- Oxidation of Si 3 N 4 Alloys: Relation to Phase Equilibria in the System Si 3 N 4 ‐SiO 2 ‐MgOJournal of the American Ceramic Society, 1980
- Characterization of large ceramic billets for core support and thermal insulaton in the HTGR1979
- Kinetics of Oxidation of Hot‐Pressed Silicon Nitride Containing MagnesiaJournal of the American Ceramic Society, 1978
- Phase Relations in the System Si 3 N 4 ‐SiO 2 ‐MgO and Their Interrelation with Strength and OxidationJournal of the American Ceramic Society, 1978
- Oxidation of Si 3 N 4 in the Range 1300 ° to 1500 ° CJournal of the American Ceramic Society, 1976
- Thermodynamics and kinetics of oxidation of hot-pressed silicon nitrideJournal of Materials Science, 1976
- Oxidation Behavior of Hot‐Pressed Si 3 N 4Journal of the American Ceramic Society, 1975
- Active to passive transition in the oxidation of SiCCorrosion Science, 1971
- Passivity during the Oxidation of Silicon at Elevated TemperaturesJournal of Applied Physics, 1958