Abstract
In this study, boron-doped apatite-type lanthanum silicate powders (La9.33Si6−xBxO26−0.5x) were successfully synthesized at 600°C via the urea‒nitrate combustion method. High-conductivity solid electrolytes were obtained by sintering at 1500°C, and the effects of B3+ doping at silicon sites on the material structure were investigated. Optimization of the sintering temperature revealed that samples sintered at 1500°C exhibited a shrinkage rate, with a uniform grain size and no pores. The smaller B3+ ions successfully replaced larger Si4+ ions, leading to lattice contraction and a reduction in the unit cell volume from 587.83 ų to 584.36 ų. IR analysis revealed that the infrared vibration peaks of Si-O bonds shifted to higher wavenumbers due to B3+ doping, confirming that B3+ substituted Si4+ in the form of [BO4] tetrahedra. XPS results demonstrated an increased oxygen vacancy concentration and enhanced covalency of Si–O bonds via charge compensation effects. Electrochemical impedance tests indicated that when the B3+ doping amount reached x = 0.4, the material achieved the highest ionic conductivity of 1.14×10− 3 S/cm at 600°C. This study reveals the conductivity enhancement mechanism through B3+ doping-induced oxygen vacancy formation, which accelerates ion migration, providing a theoretical basis for developing high-performance intermediate-temperature solid oxide fuel cell electrolytes.

This publication has 26 references indexed in Scilit: