Abstract
We investigate the practically used pipes for water supply and drain at an underground facility. The cavities are observed on the inside surface of supply pipe, whereas uniform corrosion is generally observed on the other surface. On the other hands, hematite Fe2O3 is detected at the outside surfaces on both supply and drain pipes. Though Fe2O3 is formed on the inside surface of supply pipe, Fe3O4 is formed on the inside surface of drain pipe. Electrochemical measurement reveals that the corrosion potential of the inside surface of drain pipe shows higher level. This shows that the alkali elements at the environment works as a corrosion prevent matter for drain pipe.