Design of Boiler Welding for Improvement of Lifetime and Cost Control
Open Access
Abstract
Fe-2.25Cr-1Mo a widely used material for headers and steam tubes of boilers. Welding of steam tube to header is required for production of boiler. Heat affected zone of the weld can have poor mechanical properties and poor corrosion behavior leading to weld failure. The cost of material used for steam tube and header of boiler should be controlled. This study propose a new materials design for boiler welding to improve the lifetime and cost control, using tungsten inert gas (TIG) welding of Fe-2.25Cr-1Mo tube to carbon steel pipe with chromium-containing filler. The cost of production could be reduced by the use of low cost material such as carbon steel pipe for boiler header. The effect of chromium content on corrosion behavior of the weld was greater than that of the microstructure. The lifetime of the welded boiler can be increased by improvement of mechanical properties and corrosion behavior of the heat affected zone.Keywords
This publication has 32 references indexed in Scilit:
- Change of precipitate free zone during long-term creep in 2.25Cr–1Mo steelMaterials Science and Engineering: A, 2014
- Microstructural study and electrochemical behavior of low alloy steel weldmentMaterials & Design (1980-2015), 2010
- Electrochemical frequency modulation and inductively coupled plasma atomic emission spectroscopy methods for monitoring corrosion rates and inhibition of low alloy steel corrosion in HCl solutions and a test for validity of the Tafel extrapolation methodCorrosion Science, 2009
- Finite element analysis of temperature field, microstructure and residual stress in multi-pass butt-welded 2.25Cr–1Mo steel pipesComputational Materials Science, 2008
- Corrosion and its inhibition in SA213-T22 TIG weldments used in power plants under neutral and alkaline environmentsMaterials Science and Engineering: A, 2006
- Effect of reheating processes on grain boundary heritance for 2.25Cr–1Mo–0.25V steelMaterials Science and Engineering: A, 2006
- Microstructural degeneration of simulated heat-affected zone in 2.25Cr–1Mo steel during high-temperature exposureMaterials Science and Engineering: A, 2003
- A quantitative X-ray diffraction and analytical electron microscopy study of service-exposed 2.25Cr–1Mo steelsMaterials Characterization, 2001
- Some applications of analytical TEM to the characterisation of high temperature equipmentMicron, 2001
- Microstructure of heat resistant chromium steel weld metalsApplied Surface Science, 1995