High Potential Excursions during PEM Fuel Cell Operation with Dead-Ended Anode
Open Access
- 30 July 2015
- journal article
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 162 (10) , F1212-F1220
Abstract
Operating a proton exchange membrane (PEM) fuel cell with a dead-ended anode may lead to local fuel starvation due to the excessive accumulation of liquid water and possibly nitrogen (because of membrane crossover) in the anode compartment. In this paper, we present experimental results obtained with a segmented, linear cell with reference electrodes along the gas channels, used to record local anode and cathode potentials. By simultaneously monitoring the local potentials and current densities during operation, we assessed the impact of fuel starvation on local fuel cell performance during aging protocols consisting of repeated dead-ended anode operation sequences (with anode outlet closed longer than in real use conditions). During the aging protocols, we observed strong local cathode potential excursions close to the anode outlet. The cathode showed non-uniform ElectroChemical Surface Area (ECSA) losses and performance degradation along the cell area. The damage was more severe in the regions suffering the longest from fuel starvation. Similar experiments performed in different operating conditions and with different membrane thickness showed that water management impacts significantly the cathode potential variations and thus the MEA degradation. Most of the MEA degradation is attributed to local cathode potential excursions above 1.2 V although potential cycling between 0.5 V and 0.7 V also had an impact in the regions well supplied with hydrogen (hydrogen purges were triggered when the fuel cell voltage dropped from about 0.7 V to 0.5 V). According to our results, localized and transient hydrogen starvation events may be difficult to detect by considering only the overall fuel cell performance.Keywords
This publication has 31 references indexed in Scilit:
- Experimental characterization of internal currents during the start-up of a proton exchange membrane fuel cellJournal of Power Sources, 2011
- Properties of Nafion membranes under PEM water electrolysis conditionsInternational Journal of Hydrogen Energy, 2011
- Carbon Corrosion in PEM Fuel Cell Dead-Ended Anode OperationsJournal of the Electrochemical Society, 2011
- In situ comparison of water content and dynamics in parallel, single-serpentine, and interdigitated flow fields of polymer electrolyte membrane fuel cellsJournal of Power Sources, 2010
- Effects of Cathode Inlet Relative Humidity on PEMFC Durability during Startup–Shutdown CyclingJournal of the Electrochemical Society, 2010
- Measuring oxygen, carbon monoxide and hydrogen sulfide diffusion coefficient and solubility in Nafion membranesElectrochimica Acta, 2009
- An experimental study on water transport through the membrane of a PEFC operating in the dead-end modeInternational Journal of Hydrogen Energy, 2009
- Carbon support oxidation in PEM fuel cell cathodesJournal of Power Sources, 2008
- Measurement of Liquid Water Accumulation in a PEMFC with Dead-Ended AnodeJournal of the Electrochemical Society, 2008
- Experimental investigation of liquid water formation and transport in a transparent single-serpentine PEM fuel cellJournal of Power Sources, 2007