The Influence of Cu Powders Doping on Magnetic and Mechanical Properties of Sm₂Co₁₇ Permanent Magnets
- 19 July 2024
- journal article
- research article
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Magnetics
- Vol. 60 (10) , 1-5
Abstract
In this work, the influence of Cu powders doping on the magnetic and mechanical properties of Sm 2 Co 17 permanent magnets is systematically investigated. For high-energy-product Sm 2 Co 17 (low initial Cu content), the intrinsic coercivity is significantly improved from 11.7 kOe to 25.7 kOe with 1 wt.% Cu powders doping. The flux loss (soaking at 300 °C for 2 h) is reduced from 7.4% to 3.8%, and the average flexure strength is improved from 60.2 MPa to 74.1 MPa. As for high-temperature-resistant Sm 2 Co 17 (high initial Cu content), the intrinsic coercivity is slightly reduced from 39.2 kOe to 38.3 kOe with 1 wt.% Cu powders doping. The flux loss (soaking at 300 °C for 2 h) is increased from 1.4% to 3.4%, and the average flexure strength is improved from 86.7 MPa to 93.2 MPa. The differences in magnetic properties change of these two Sm 2 Co 17 permanent magnets are closely related with their initial Cu content. The doped Cu is prone to diffuse into intragranular cell boundaries in magnet with low initial Cu content. The increased Cu content in intragranular cell boundaries benefits the improvement of intrinsic coercivity, thus enhancing the thermal stability and reducing the flux loss. Doping Cu powders may increase the Cu-rich phase around ground boundaries, which will hinder the grain growth during heat treatment. The decrease of grain size will enhance the flexure strength, while it will increase the flux loss.Keywords
Funding Information
- National Key Research and Development Program of China (2021YFB3503101)
- Natural Science Foundation of Ningbo Municipality (2023J347)
- Youth Innovation Promotion Association Chinese Academy of Sciences (2023311)
This publication has 30 references indexed in Scilit:
- Effect of interfacial stress on microchemistry and coercivity in 2:17-type SmCo sintered magnetsActa Materialia, 2023
- Study on the grain growth and the evolution of defects around grain boundaries during heat treatment process in Sm2Co17 permanent magnetsJournal of Alloys and Compounds, 2023
- Atomic‐Scale Transition Zones Determined Coercivity in Samarium‐Cobalt Based Permanent MagnetsAdvanced Functional Materials, 2023
- In-situ high-energy X-ray diffraction study of the early-stage decomposition in 2:17-type Sm-Co-based permanent magnetsActa Materialia, 2022
- The influence of final aging temperature on thermal stability of microstructure and magnetic properties in Sm(Co,Fe,Cu,Zr)z high temperature magnetsJournal of Alloys and Compounds, 2022
- Atomic-scale structure clarification of the planar Z phase and its influence on the magnetic properties in Sm(CoFeCuZr) permanent magnetsActa Materialia, 2022
- Fe content influence on the microstructure of solution-treated Sm-Co-Fe-Cu-Zr alloysIntermetallics, 2021
- Grain boundary effect on the microstructure of solution-treated Fe-rich Sm-Co-Fe-Cu-Zr alloysJournal of Alloys and Compounds, 2021
- Attractive-domain-wall-pinning controlled Sm-Co magnets overcome the coercivity-remanence trade-offActa Materialia, 2019
- The microstructure of sintered Sm(Co0.72Fe0.20Cu0.055Zr0.025)7.5 permanent magnet studied by atom probeActa Materialia, 2004