Effects of La 2 O 3 /ZnO Additives on Microstructure And Microwave Dielectric Properties of Zr 0.8 Sn 0.2 TiO 4 Ceramics

Authors:

Abstract
Dielectric ceramics of Zr 0.8 Sn 0.2 TiO 4 containing La 2 O 3 and ZnO as sintering aids were prepared and investigated for microstructure and microwave dielectric properties. Low‐level doping with La 2 O 3 and ZnO (up to 0.30 wt%) is good for densification and dielectric properties. These additives do not affect the dielectric constant and the temperature coefficient. Dielectric losses increase significantly at additive levels higher than 0.15 wt%. The combined additives La 2 O 3 and ZnO act as grain growth enhancers. With 0.15 wt% additives, a ceramic having a dielectric constant, a quality factor, and a temperature coefficient of frequency at 4.2 GHz of 37.6, 12 800, and –2.9 ppm/°C, respectively, was obtained. The quality factor was considerably improved by prolonged sintering.