Sintering of Zinc Oxide Doped with Antimony Oxide and Bismuth Oxide

Authors:

Abstract
The phase change, densification, and microstructure development of ZnO doped with both Bi 2 O 3 and Sb 2 O 3 are studied to better understand the sintering behavior of ZnO varistors. The densification behavior is related to the formation of pyrochlore and liquid phases; the densification is retarded by the former and promoted by the latter. The pyrochlore phase, whose composition is Bi 3/2 ZnSb 3/2 O 7 , appears below 700°C. The formation temperature of the liquid phase depends on the Sb/Bi ratio: about 750°C for Sb/Bi < 1 by the eutectic melting in the system ZnO—Bi 2 O 3 , and about 1000°C for Sb/Bi > 1 by the reaction of the pyrochlore phase with ZnO. Hence, the densification rate is determined virtually by the Sb/Bi ratio and not by the total amount of additives. The microstructure depends on the sintering temperature. Sintering at 1000°C forms intragrain pyrochlore particles in ZnO grains as well as intergranular layers, but the intragrain particles disappear at 1200°C by the increased amount of liquid phase, which enhances the mobility of the solid second phase.

This publication has 9 references indexed in Scilit: