Melt fracture behavior of polypropylene‐type resins with narrow molecular weight distribution. II. Suppression of sharkskin by addition of adhesive resins
- 19 March 2002
- journal article
- research article
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 84 (12) , 2120-2127
Abstract
No abstract availableKeywords
This publication has 18 references indexed in Scilit:
- Melt fracture behavior of polypropylene‐type resins with narrow molecular weight distribution. I. Temperature dependenceJournal of Applied Polymer Science, 2002
- Disappearance of extrusion instabilities in brass capillary diesJournal of Rheology, 1999
- The effect of teflon™ coatings in polyethylene capillary extrusionJournal of Applied Polymer Science, 1995
- Sharkskin defects of polymer melts: The role of cohesion and adhesionJournal of Rheology, 1991
- Additional observations on the surface melt fracture behavior of linear low-density polyethyleneJournal of Non-Newtonian Fluid Mechanics, 1990
- The different capillary flow regimes of entangled polydimethylsiloxane polymers: macroscopic slip at the wall, hysteresis and cork flowJournal of Non-Newtonian Fluid Mechanics, 1990
- Influence of upstream instabilities and wall slip on melt fracture and sharkskin phenomena during silicones extrusion through orifice diesJournal of Non-Newtonian Fluid Mechanics, 1990
- Wall Slip and Extrudate Distortion in Linear Low‐Density PolyethyleneJournal of Rheology, 1987
- Wall Slip in Viscous Fluids and Influence of Materials of ConstructionJournal of Rheology, 1986
- Stretching flow instabilities at the exits of extrusion diesJournal of Non-Newtonian Fluid Mechanics, 1977