Formation of Mullite Coating by Aerosol Deposition and Microstructural Change after Heat Exposure
Authors:
- 1 March 2020
- journal article
- research article
- Published by Japan Institute of Metals in MATERIALS TRANSACTIONS
- Vol. 61 (3) , 540-547
Abstract
Optimal parameters for the aerosol deposition (AD) of a mullite coating and the microstructural change of the coating after heat exposure in air were investigated. Mullite, which is a component of environmental barrier coatings, was deposited on glass, Al2O3 and Si by the AD method. The angle of the gas flow direction from the nozzle to the substrate plane should be 60° to produce a homogeneous mullite coating. The deposition rate increased with the gas flow rate when the gas flow rate was in the range from 18 to 36 L/min. Further increase of the gas flow rate resulted in the formation of a heterogeneous coating. The mullite coating formed with the optimized parameters was almost fully dense and crystalline. The chemical composition of the mullite coating was almost the same as that of the raw mullite powder used for deposition. The coating was composed of a single mullite phase. No delamination was observed at the interface between the Si substrate and the mullite coating. The interface did have undulations; therefore, it was considered that the substrate and the coating were bonded due to the anchor effect. Heat treatment was performed at 1573 K for a mullite coating deposited on a Si substrate. When the specimen was exposed to heat for 10 h, the coating at the surface side and the coatings at the central part and near the interface between the substrate and the coating were composed of two phases, (Al2O3+mullite) and (SiO2+mullite), respectively. Further heat exposure results in the formation of a reacted layer of two phases (SiO2+mullite) containing more than 80 mol% of SiO2 near the interface. The thickness of the layer increased with increasing heat exposure time. The formation of the reacted layer was due to the diffusion of Al present in the mullite coating to the coating surface and the diffusion of Si into the coating from the Si substrate. This Paper was Originally Published in Japanese in J. Japan Inst. Met. Mater. 83 (2019) 186–192.Keywords
This publication has 31 references indexed in Scilit:
- Effect of Process Gas Flow on the Coating Microstructure and Mechanical Properties of Vacuum Kinetic-Sprayed TiN LayersJournal of Thermal Spray Technology, 2013
- Growth Process of α‐Al2O3 Ceramic Films on Metal Substrates Fabricated at Room Temperature by Aerosol DepositionJournal of the American Ceramic Society, 2011
- Appearance of high-temperature phase in zirconia films made by aerosol gas deposition methodJournal of the Ceramic Society of Japan, 2011
- Formation of zirconia films by the aerosol gas deposition methodJournal of the Ceramic Society of Japan, 2010
- Formation of zirconia films by aerosol gas deposition method using zirconia powder produced by break-down methodJournal of the Ceramic Society of Japan, 2010
- Gas Permeability of Oxide Ceramics at Ultra-High TemperaturesJournal of the Society of Materials Science, Japan, 2008
- Aerosol Deposition of Ceramic Thick Films at Room Temperature: Densification Mechanism of Ceramic LayersJournal of the American Ceramic Society, 2006
- Room Temperature Impact Consolidation of Ceramic Particles on Aerosol Deposition and Its applicationsJOURNAL OF THE JAPAN WELDING SOCIETY, 2006
- Oxidation and Volatilization of Silica Formers in Water VaporJournal of the American Ceramic Society, 2003
- Stable and Metastable Equilibria in the System SiO 2 ‐Al 2 O 3Journal of the American Ceramic Society, 1975