Improvement in Surface Grinding Damage in Silicon Wafers by Chemical Spin Etching
Author:
- 24 January 2014
- journal article
- Published by The Electrochemical Society in ECS Journal of Solid State Science and Technology
- Vol. 3 (4) , Q61-Q64
Abstract
Understanding damage caused by mechanical grinding is required for wafer thinning processes, because such damage significantly affects device performance in large-scale integrated circuits. Herein, in-depth analysis of damage caused by mechanical grinding was conducted by measuring minority carrier lifetime and by the photoacoustic displacement (PAD) technique, which are highly sensitive and quantitative methods for measuring damage. Previous low-sensitivity damage measurements indicate that grinding damage is distributed within a 5-μm-thick surface layer. However, although a 10-μm-thick surface layer is removed by chemical spin etching (CSE), the minority carrier lifetime remains low. This result suggests that significant damage still exists in layers deeper than 10 μm. After etching a 200-μm-thick layer, PAD measurements show that displacement at the surface recovers to 20 pm, which is the level of undamaged silicon. While minority carrier lifetime gradually increases with increased etching, this lifetime remains low after removing a 100-μm-thick strain layer. The minority carrier lifetime reaches that of defect-free silicon after removing a 300-μm-thick layer. These results clearly indicate that deep damage (i.e., depth of 200 μm) is caused at the silicon surface by conventional mechanical grinding. Additionally, we conclude that the CSE process is useful for thinning silicon wafers without inducing damage or strain.Keywords
This publication has 17 references indexed in Scilit:
- Iron detection in crystalline silicon by carrier lifetime measurements for arbitrary injection and dopingJournal of Applied Physics, 2004
- Role of inversion layer formation in producing low effective surface recombination velocities at Si/liquid contactsApplied Physics Letters, 2000
- Contactless mapping of lifetime and diffusion length scan map of minority carriers in silicon wafersThe European Physical Journal Applied Physics, 2000
- Monitoring and Optimization of Silicon Surface QualityJournal of the Electrochemical Society, 1995
- Characteristics of photoacoustic displacement for silicon damaged by ion implantationJournal of Applied Physics, 1995
- Analysis of lattice defects induced by ion implantation with photo-acoustic displacement measurementsJournal of Applied Physics, 1994
- Theoretical Analysis of Photoacoustic Displacement for Inhomogeneous MaterialsJapanese Journal of Applied Physics, 1994
- Effects of ambient gas and temperature on photo-acoustic displacement for semiconductorsOptical Review, 1994
- Photoconductance Minority Carrier Lifetime vs. Surface Photovoltage Diffusion Length In SiliconJournal of the Electrochemical Society, 1993
- In situ bulk lifetime measurement on silicon with a chemically passivated surfaceApplied Surface Science, 1993