Abstract
Extensively use of hot-curing acrylic in prosthetic dentistry field, increase the needed to modifying its mechanical, thermal, and physical properties. In this work Yttrium oxide had added with different weight fractions, (5%, 10%, 15% and 20%), as reinforcement phase on purpose of developing these properties. Tensile strength, hardness, density, water adsorption, and thermal conductivity had been investigated for prepared composite specimens. The results show that the maximum tensile strength was at (10) % wt. of Y2O3 addition, (19) %more than that of plain acrylic, maximum hardness was at (15) % wt. of Y2O3 addition, (8.5) % more than that of plain acrylic, maximum density was at (20) % wt. of Y2O3 addition, (18.2) % more than that of plain acrylic, maximum decrease in water absorption was at (10) % wt. of Y2O3 addition, (29) % less than that of plain acrylic. Finally the maximum thermal conductivity was at (20) % wt. of Y2O3 addition, (16) % more than that of plain acrylic.