The Effect of a Deproteinizing Pretreatment on the Bonding Performance and Acid Resistance of a Two-step Self-etch Adhesive on Eroded Dentin
Authors:
- 1 January 2024
- journal article
- research article
- Published by Operative Dentistry in Operative Dentistry
- Vol. 49 (1) , 65-75
Abstract
SUMMARY: Objectives: This study evaluated how deproteinization using sodium hypochlorite (6% NaOCl) or hypochlorous acid (50 ppm HOCl) with or without the subsequent use of an arylsulfinate salt-containing agent (Clearfil DC Activator; DCA; Kuraray Noritake Dental) affects the micro-tensile bond strength (μTBS) and formation of an acid-base resistant zone (ABRZ) of a two-step self-etch adhesive on eroded dentin. Methods: Coronal dentin surfaces of sound human molars were exposed to 48 cycles of demineralization (1% citric acid; 5 minutes) and remineralization (buffer solution with pH=6.4; 3.5 hours). They were then assigned to experimental groups according to the pretreatment used: none (negative control), NaOCl, NaOCl+DCA, HOCl, and HOCl+DCA. Sound dentin surfaces with no pretreatment were used as a positive control. The dentin surfaces were bonded with Clearfil SE Bond 2 (Kuraray Noritake Dental), and μTBS was measured either after 24 hours or 20,000 thermal cycles (TC). The μTBS data were statistically analyzed using a mixed-model analysis of variance (ANOVA) and t-tests with Bonferroni correction. Failure mode was determined with scanning electron microscopy (SEM), which was also used for the observation of ABRZ. Results: Among experimental groups, there was no significant difference between the negative control, HOCl, and HOCl+DCA after 24 hours, but the HOCl-pretreated groups exhibited significantly higher μTBS than the negative control after TC (p<0.01). Pretreatment with NaOCl and NaOCl+DCA resulted in significantly higher μTBS (p<0.001), but the highest μTBS was measured on sound dentin (p<0.001). TC decreased μTBS significantly in all groups (p0.05). Adhesive failures prevailed in eroded groups, whereas cohesive failures were predominant on sound dentin. ABRZ was recognized in all groups but marked morphological differences were observed. Conclusions: The combined use of 6% NaOCl and the arylsulfinate salt-containing agent partially reversed the compromised bonding performance on eroded dentin, while the effect of 50 ppm HOCl was negligible.Keywords
This publication has 47 references indexed in Scilit:
- Effect of antioxidant/reducing agents on the initial and long-term bonding performance of a self-etch adhesive to caries-affected dentin with and without smear layer-deproteinizingInternational Journal of Adhesion and Adhesives, 2020
- Smear layer-deproteinizing improves bonding of one-step self-etch adhesives to dentinDental Materials, 2018
- Apatite crystal protection against acid-attack beneath resin–dentin interface with four adhesives: TEM and crystallography evidenceDental Materials, 2012
- The effect of a tin-containing fluoride mouth rinse on the bond between resin composite and erosively demineralised dentinClinical Oral Investigations, 2012
- Long-term bonding to eroded dentin requires superficial bur preparationClinical Oral Investigations, 2011
- Effect of reducing agents on bond strength to NaOCl-treated dentinDental Materials, 2011
- State of the art of self-etch adhesivesDental Materials, 2011
- Assessment and Management of Dental ErosionDental Clinics of North America, 2010
- Dental adhesion review: Aging and stability of the bonded interfaceDental Materials, 2008
- Elemental distributions and microtensile bond strength of the adhesive interface to normal and caries‐affected dentinJournal of Biomedical Materials Research Part B: Applied Biomaterials, 2004