Abstract
A series of solid complexes, PEI−PFAO, made of poly(ethylenimine) (PEI) and perfluorooctanoic acid (PFOA) with different compositions were prepared through a “starving addition” method, where PFOA was fed into PEI solution at the molar ratio, φfeed, of acid group to the amino group of PEI, never beyond unity. Wide-angle X-ray diffraction diagrams confirmed amorphous structure of these complexes. Small-angle X-ray scattering indicated two ordered mesomorphous structures of α and β lamellar phases, with respective long periods of 2.29 and 1.15 nm in the complexes. By increasing the actual molar ratio, φ, of PFOA to the amino group of PEI, the complex structure was altered from α-phase dominant to β-phase dominant. All complexes exhibited two thermal degradation processes induced by decomposition of the bound PFOA below 230 °C and PEI backbone at about 350 °C. The initiating degradation temperature, Tid, decreases with increasing φ due to the preferential degradation of the PFOA chain bound to the tertiary amino groups. The glass transition temperature, Tg, of the complex increases with φ up to the degradation of the complex of φ = 1. This increase in Tg with φ also supports an ordered alignment of the bound PFOA chains, which greatly restricts the PEI mobility. The solid surface tension, γS, and critical surface tension, γc, of the complex are between 15.4 and 16.8 mN/m and between 13.5 and 15.4 mN/m, respectively. The latter is very close to or even smaller than γc of PTFE (15 mN/m), suggesting the enrichment of CF2 and CF3 groups at the complex surfaces. The fact that the PEI−POFA complex combines high hydrophobicity with selective thermal degradation of bound fluorinated chains promises a potential of selective change and local functionalization of the surface in a well-controlled manner.

This publication has 34 references indexed in Scilit: