Synergistic Effects of Guide Tube Configuration and Heating Ramp Rate on the Quality of Large‐Scale 8‐inch 4H‐SiC Crystals

Authors:

Abstract
We systematically evaluated how the graphite inner guide tube‐to‐seed distance (D) as well as the heating ramp rate (S), impact seed stability during the initial stages and the final 8‐inch n ‐type 4H‐SiC single crystal quality using the PVT (Physical vapor transport) method. We found that a specific distance of approximately 8 mm minimizes the damage width (DW) of the seed crystal by balancing the radial temperature gradient and stabilizing the SiC source vapor flow. In addition, a heating ramp rate (S) of 3–6°C/min was selected as the optimal regime to rapidly establish a stable thermal field, effectively suppressing microcrack initiation and polytype inclusions. By applying these optimized conditions, 8‐inch n ‐type 4H‐SiC crystals with remarkably low defect densities were successfully grown. Our measurements confirmed micropipe densities below 1 ea/cm 2 , threading screw dislocation (TSD) densities below 500 ea/cm 2 , and basal plane dislocation (BPD) densities less than 1,000 ea/cm 2 . These parameters establish a practical guideline for the design of hot‐zone configuration and thermal protocols for the reliable and consistent production of large‐scale SiC crystals.

This publication has 14 references indexed in Scilit: