Abstract
This paper describes the successful development of the co-precipitation technique for the preparation of a high-sensitive dysprosium-doped calcium sulphate (CaSO4:Dy) thermoluminescent dosimetry (TLD) phosphor with dosimetric glow peak at ∼230°C which is a desired development in the field of radiation protection dosimetry. The main advantages of this co-precipitation technique over the conventional recrystallisation technique of phosphor preparation are: (i) preparation time is very less; (ii) quantity of sulphuric acid evaporated is insignificant; (iii) higher TL sensitivity −20% more than the present material; (iv) better glow curve structure; (v) lesser glow peak shift and better linearity to gamma and (vi) uniform crystal morphology and lower grain size—all grains are mostly cuboidal in shape, quite uniform and small (average size about 25 µm), suitable for manufacturing teflon discs in as-prepared form. Optimum values of various parameters in the method of preparation for a batch of 20 g CaSO4:Dy phosphors to obtain maximum TL sensitivity, with favourable glow curves are studied.

This publication has 9 references indexed in Scilit: