Tensile strength of synthetic chemical-vapor-deposited diamond
Authors:
- 15 October 1995
- journal article
- conference paper
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 78 (8) , 5177-5179
Abstract
Pressure burst tests gave measured tensile strengths between 230 and 410 MPa for a total of six chemical‐vapor‐deposited (CVD) diamond disks in both transparent ‘‘white’’ and opaque ‘‘black’’ forms obtained from three different sources. The disks were nominally 0.635 cm in diameter and 254 μm thick. These strengths are explained by a theoretical model using a Young’s modulus of 1.05×106 MPa and a fracture surface energy of 5.3 J/m2, appropriate for natural diamond, and with critical crack lengths between 33 and 105 μm. The latter lengths can fit, either on or inside, the tapered columnar crystal grains that grow vertically in synthetic CVD diamond films. The model is consistent with the observed inverse dependence of measured tensile strength on film thickness and with tensile strengths between 180 and 5190 MPa reported by other workers for synthetic CVD diamond.Keywords
This publication has 8 references indexed in Scilit:
- Properties of diamond for window and dome applications1994
- Linewidths of phonon lines of natural and synthetic diamondsApplied Physics Letters, 1994
- Fracture surface analysis of free-standing diamond filmsJournal of Materials Research, 1994
- Mechanical Properties of Diamond MembranesJapanese Journal of Applied Physics, 1993
- Fracture strength measurement of filament assisted CVD polycrystalline diamond filmsJournal of Materials Research, 1992
- Unusually high thermal conductivity in diamond filmsApplied Physics Letters, 1992
- Fracture Toughness of Chemically Vapor‐Deposited DiamondJournal of the American Ceramic Society, 1991
- The history and present status of synthetic diamondJournal of Crystal Growth, 1979