Direct recycling of EV production scrap NMC532 cathode materials
Open Access
- 4 September 2024
- journal article
- research article
- Published by Royal Society of Chemistry (RSC) in RSC Sustainability
- Vol. 2 (10) , 3014-3021
Abstract
The transition to widespread adoption of electric vehicles (EVs) is leading to a steep increase in lithium ion battery production around the world. With this increase it is predicted there will not only be a large increase in end of life batteries needing to be recycled, but also a substantial amount of production scrap, particularly in the early stages of gigafactory set-up. The recycling of such battery electrode materials has a number of challenges which need to be considered, in particular the delamination from the current collector and removal of the binder, e.g. mainly polyvinylidene fluoride (PVDF) for cathode materials. Traditional pyrometallurgy or hydrometallurgy approaches require multiple separation steps to obtain pure metal salts before resynthesising the cathode active material, and so can be high cost, high CO2 and high waste processes. Production scrap in particular, however, offers the potential for lower cost and lower environmental impact direct recycling processes to be employed, which preserves the manufactured value of the electrode material. To illustrate the potential of such an approach, here we demonstrate a direct recycling approach on EV production scrap cathode materials which utilises a low temperature heat treatment to decompose the binder and allow delamination of the cathode material from the Al current collector. A further higher temperature heat treatment is then employed to ensure complete binder removal and regenerate the cathode, with the results showing that the addition of a small amount of Li is required to improve electrochemical performance (first cycle discharge capacity (2.5–4.2 V) of 129(2) mA h g−1 and 146(4) mA h g−1 with 0 wt% and 10 wt% added lithium, respectively). Electrochemical performance can be further improved by increasing the upper voltage window to 4.3 V (first cycle discharge capacity of 146(4) mA h g−1 and 164(2) mA h g−1 at 2.5–4.2 V and 2.5–4.3 V, respectively).Keywords
Funding Information
- Faraday Institution (FIRG005, FIRG015, FIRG016, FIRG027, FIRG057, FIRG063)
This publication has 32 references indexed in Scilit:
- Phase-selective recovery and regeneration of end-of-life electric vehicle blended cathodes via selective leaching and direct recyclingJoule, 2024
- Towards Greener Recycling: Direct Repair of Cathode Materials in Spent Lithium-Ion BatteriesElectrochemical Energy Reviews, 2024
- Direct and rapid regeneration of spent LiFePO4 cathodes via a high-temperature shock strategyJournal of Power Sources, 2023
- Direct recycling of degraded lithium-ion batteries of an electric vehicle using hydrothermal relithiationMaterials Today Energy, 2023
- Direct reuse of oxide scrap from retired lithium‐ion batteries: advanced cathode materials for sodium‐ion batteriesRare Metals, 2023
- Insights into architecture, design and manufacture of electrodes for lithium-ion batteriesMaterials & Design, 2022
- Concurrent recycling chemistry for cathode/anode in spent graphite/LiFePO4 batteries: Designing a unique cation/anion-co-workable dual-ion batteryJournal of Energy Chemistry, 2022
- A qualitative assessment of lithium ion battery recycling processesResources, Conservation and Recycling, 2021
- The structural mechanism of the improved electrochemical performances resulted from sintering atmosphere for LiNi0.5Co0.2Mn0.3O2 cathode materialJournal of Alloys and Compounds, 2013
- Effects of synthesis conditions on the structural and electrochemical properties of layered Li[Ni1/3Co1/3Mn1/3]O2 cathode material via the hydroxide co-precipitation method LIB SCITECHJournal of Power Sources, 2006