Dielectric behavior of Cd 2 Nb 2 O 7 has been studied from room temperature down to 10 K with and without dc electric fields. Three dielectric relaxation modes I, II, and III were reexamined. By using the Cole - Cole equation fitting of the frequency dependence of the dielectric constant and loss of Cd 2 Nb 2 O 7 , we have obtained more precise relaxation time data, compared to the data reported in the literature. The results indicate that the relaxation time follows both the Arrhenius law and Vogel - Fulcher relation in the frequency range of 10 2 - 10 5 Hz. With increasing dc bias, the relaxation modes were suppressed and eventually eliminated. The results show a significant suppression of the dielectric constant and loss by the application of dc fields. At above 10 kV/cm, only a dielectric peak remains. The high tunability (37 - 64%) under 15 kV/cm at 5 kHz in the wide temperature range of 50 - 180 K and very low dielectric loss (0.4 - 6 2 10 m 3 )) are observed.