Hot‐Pressing Magnesium Fluoride
Authors:
- 1 September 1962
- journal article
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 45 (9) , 435-438
Abstract
Hot‐pressing powdered magnesium fluoride resulted in a polycrystalline compact with essentially the density and transmittance of a single crystal. Compacted powdered MgF2 was heated to 650°C and held under a pressure of 30,000 psi for 15 minutes. The starting material had to be free from impurities which would form a second phase, and the presence of water and bound hydroxyl groups had to be minimized. Overheating caused the starting material to resist hot‐pressing. It is postulated that mechanical bulk decrease was followed by plastic deformation during pressing and that both solid and surface diffusion of material took place to complete the coalescence of the grains.Keywords
This publication has 3 references indexed in Scilit:
- Some Properties of Magnesium Fluoride crystallized from the MeltProceedings of the Physical Society (1958-1967), 1958
- Cases and CommentsThe Journal of the American Dental Association, 1957
- The Resistance of 72 Elements, Alloys and Compounds to 100,000 Kg/Cm²Proceedings of the American Academy of Arts and Sciences, 1952