Abstract
Pulse electric current sintering is used to prepare a compact from resinificated hydrous silk powder. Compacts with no remnant silk powders are formed with 20 wt% added water, 20–40 MPa molding pressure, and >353 K molding temperature. The latter two are much lower than those used for conventional hot pressing. No dependence on molding pressure and temperature are found in XRD or FT‐IR analysis, except for a compact molded at 473 K, for which silk fibroin decomposition is confirmed by DSC, EGA‐MS, and molecular weight measurements. The compact's three‐point bending strength depends on the molding temperature, except for the temperature at which silk fibroin decomposes. The maximum three‐point bending strength resembles that of general‐purpose epoxy resin and is much higher than that of PLA. magnified image