Enhancing tribological performance of Ti-6Al-4V by sliding process
- 8 June 2018
- journal article
- research article
- Published by SAGE Publications in Tribology - Materials, Surfaces & Interfaces
- Vol. 12 (3) , 137-143
Abstract
The exceptional combination of mechanical, physical and anti-corrosive properties of Titanium alloy Ti-6Al-4 V (Ti64) makes it idle material for the applications like aerospace, automobile, chemical, medical etc. However, Ti64 exhibits poor tribological (friction and wear) properties, which limits its implementation in the intended applications. The tribological performance of the Ti64 can be enhanced by developing a protective layer or coating on its surface. It has been reported in literatures that through rubbing process the oxide layers can be achieved at much lower temperature compared to external heating process. Therefore, an endeavour is made in the present work to achieve a tribo-oxide protective layer on the surface of Ti64 through rubbing process. For this, at first the tribological behaviour of tribo pair: Ti64 pin-alumina disc is studied under dry ambient condition for diverse loading and sliding speed conditions, using pin on disc experimental set-up. The obtained results are compared with literatures. The tribological performance is quantified in terms of coefficient of friction (COF) and wear rate. To investigate the tribological mechanism and behaviour, in-situ analysis was performed on the pin’s surface using (i) scanning electron microscopy, and (ii) energy dispersive analysis of X-ray. The mechanical properties like nano-hardness and elastic modulus of the pins surface were also determined. It was envisaged that the tribological behaviour were extremely transient and depend greatly on what the surface has precisely experienced Based on the experimental observations, the experimental conditions providing (i) Case1: deprived tribological properties and (ii) Case 2: higher oxide layer is selected. Now, to enhance the tribological behaviour of Case 1, the pin with high oxide layer, i.e. Case 2 is used. For this experiment is performed initially for Case 2 conditions for the sliding distance of 1000 m (for developing oxide layer) and the experiment is continued for next 1000 m for Case 1 condition. The experimental results in terms of COF and wear rate are presented and corresponding enhancement in their values are discussed.Keywords
This publication has 34 references indexed in Scilit:
- Cellular Ti–6Al–4V structures with interconnected macro porosity for bone implants fabricated by selective electron beam meltingActa Biomaterialia, 2008
- Microstructure and tribological characteristics of Ti–6Al–4V alloy against GCr15 under high speed and dry slidingMaterials Science and Engineering: A, 2006
- Excimer laser surface treatment of Ti–6Al–4V alloy for corrosion resistance enhancementMaterials Letters, 2002
- Titanium alloys for marine applicationMaterials Science and Engineering: A, 1999
- Surface modification of titanium alloys for combined improvements in corrosion and wear resistanceSurface and Coatings Technology, 1998
- Recent developments in titanium alloy application in the energy industryMaterials Science and Engineering: A, 1998
- The use of titanium for medical applications in the USAMaterials Science and Engineering: A, 1996
- An overview on the use of titanium in the aerospace industryMaterials Science and Engineering: A, 1996
- An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experimentsJournal of Materials Research, 1992
- Improving the properties of titanium alloys by ion implantationJOM, 1990