Comparison of different kinetic models for NOX storage on a lean NOX trap
- 14 August 2014
- journal article
- research article
- Published by Wiley in The Canadian Journal of Chemical Engineering
- Vol. 92 (9) , 1506-1516
Abstract
The kinetics of NOX storage on a lean NOX trap (LNT) were studied using NOX breakthrough curves measured with a laboratory reactor. A much wider range of temperatures (125–450°C) was used than in most studies to facilitate discrimination between potential models. The breakthrough curves were run until the LNT was saturated to (i) enable NO oxidation to NO2 to be studied in the absence of NOX storage, (ii) to enable the effective NOX capacity as a function of temperature to be determined, and (iii) to provide a more demanding test for potential models.Breakthrough curves for 125 and 450°C were very similar, while curves at intermediate temperatures initially followed that for 125°C before breaking away from this curve at a point that became earlier with increasing temperature. Thus, the breakthrough curves have a temperature independent initial portion, followed by a temperature dependant portion. This was explained by there being two types of site: fast sites and slow sites. Fast sites are responsible for the initial part of the curve; both the rate of storage on these sites and the available capacity are independent of temperature. The rate of storage on slow sites, on the other hand, is temperature dependant, as is the available storage capacity. Slow sites are more abundant than fast sites. The performance of three NOX storage models for these sites was compared.The amount of NOX stored as a function of temperature was bell‐shaped. The models naturally predicted that storage was limited by kinetics at lower temperatures and nitrate stability at higher temperatures.Keywords
This publication has 46 references indexed in Scilit:
- Effect of cycle time on NH3 generation on low Pt dispersion Pt/BaO/Al2O3 catalysts: Experiments and crystallite-scale modelingChemical Engineering Journal, 2013
- Modeling the effects of Pt loading on NOx storage on Pt/BaO/Al2O3 catalystsApplied Catalysis B: Environment and Energy, 2011
- A review of NOx storage/reduction catalysts: mechanism, materials and degradation studiesCatalysis Science & Technology, 2011
- Modelling of a combined NOx storage and NH3-SCR catalytic system for Diesel exhaust gas aftertreatmentCatalysis Today, 2010
- Inverse hysteresis during the NO oxidation on Pt under lean conditionsApplied Catalysis B: Environment and Energy, 2009
- Global kinetic model for the regeneration of NO storage catalyst with CO, H2 and C3H6 in the presence of CO2 and H2OCatalysis Today, 2009
- Dynamics and selectivity of NO reduction in NO storage catalytic monolithCatalysis Today, 2008
- Detailed kinetic modeling of NOx storage and reduction with hydrogen as the reducing agent and in the presence of CO2 and H2O over a Pt/Ba/Al catalystJournal of Catalysis, 2008
- Model for NOx storage/reduction in the presence of CO2 on a Pt–Ba/γ-Al2O3 catalystJournal of Catalysis, 2007
- Overview of the Fundamental Reactions and Degradation Mechanisms of NOx Storage/Reduction CatalystsCatalysis Reviews, 2004