Influence of phase dissolution and hydrogen absorption on the stress corrosion cracking behavior of Mg-7%Gd-5%Y-1%Nd-0.5%Zr alloy in 3.5 wt.% NaCl solution
Authors:
- S.D. WangSWS.D. Wang
- D.K. XuDXD.K. Xu
- B.J. WangBWB.J. Wang
- L.Y. ShengL.Y. Sheng
- Y.X. QiaoY.X. Qiao
- En-Hou HanEHEn-Hou Han
- C. DongC. Dong
- 1 September 2018
- journal article
- research article
- Published by Elsevier in Corrosion Science
- Vol. 142, 185-200
Abstract
No abstract availableKeywords
Funding Information
- Chinese Academy of Sciences
- National Key Research and Development Program of China (2016YFB0301105, 2017YFB0702001)
- Special Foundation for the Development of Strategic Emerging Industries of Shenzen Municipality (JCYJ20170306141749970)
This publication has 75 references indexed in Scilit:
- Corrosion behaviour in salt spray and in 3.5% NaCl solution saturated with Mg(OH)2 of as-cast and solution heat-treated binary Mg–X alloys: X=Mn, Sn, Ca, Zn, Al, Zr, Si, SrCorrosion Science, 2013
- Corrosion processes of Mg–Y–Nd–Zr alloys in Na2SO4 electrolyteCorrosion Science, 2013
- Stress corrosion cracking of rare-earth containing magnesium alloys ZE41, QE22 and Elektron 21 (EV31A) compared with AZ80Materials Science and Engineering: A, 2008
- ESEM observation of the process of hydrogen generation around the micro-droplets forming on AZ91 magnesium alloyElectrochemistry Communications, 2008
- A Critical Review of the Stress Corrosion Cracking (SCC) of Magnesium AlloysAdvanced Engineering Materials, 2005
- Understanding Magnesium Corrosion—A Framework for Improved Alloy PerformanceAdvanced Engineering Materials, 2003
- Effects of Hydrogen on Semiconductivity of Passive Films and Corrosion Behavior of 310 Stainless SteelJournal of the Electrochemical Society, 1999
- Effects of Hydrogen on Pitting Susceptibility of Type 310 Stainless SteelCorrosion, 1998
- Stress Corrosion Cracking and Liquid Metal Embrittlement in Pure MagnesiumCorrosion, 1988
- Hydrogen induced delayed plasticity and crackingScripta Metallurgica, 1979