Stress Corrosion Cracking and Hydrogen-Induced Cracking in Austenitic Stainless Steel Under Mode II Loading

Authors:
  • LQL-J. Qiao
    L-J. Qiao
  • WCW-Y. Chu
    W-Y. Chu
  • CHC-M. Hsiao
    C-M. Hsiao

Abstract
Stress corrosion cracking (SCC) and hydrogen-induced cracking (HIC) of AISI 321 stainless steel (SS) under Mode II loading were investigated with notched specimens(1) The results showed that SCC in boiling MgCl2 solution initiated at the maximum normal stress site, i.e., at θ = −110 degrees, on the notch surface, rather than at the maximum shear stress site, i.e., at θ = 80 degrees, and its orientation was perpendicular to the direction of the maximum normal stress. However, HIC during dynamic charging initiated at the maximum shear stress site at high KII or at the maximum normal stress site at low KII. The normalized threshold stress intensity of SCC in MgCl2 solution of the AISI 321 steel under Mode II loading was KIISCC/KIIX = 0.19, which was much lower than that of HIC during dynamic charging, i.e., KIIH/KIIX = 0.59; where KIIX is a critical value loaded to failure in air under Mode II loading. In addition, the morphologies of the SCC fracture surface in MgCl2 solution differed from those of HIC, too. These results support the statement that SCC of austenitic SS in boiling MgCl2 solution results from the anodic path dissolution mechanism and the maximum normal stress, rather than the maximum shear stress controls SCC initiation.

This publication has 10 references indexed in Scilit: