Kinetic behavior of partially dehydroxylated kaolinite
Authors:
- 1 April 2015
- journal article
- Published by Mineralogical Society of America in American Mineralogist: Journal of Earth and Planetary Materials
- Vol. 100 (4) , 883-896
Abstract
The multi-cycle heating and cooling thermogravimetric (TG) method was used to study the kinetic behavior of three kaolinite samples: defect-free Keokuk kaolinite, KGa-2 with a very low degree of structural order, and KGa-1 having intermediate structural order. In each cycle, the maximum cycle temperature (MCT) was set to 25 °C higher than the preceding cycle. The TG patterns consist of a set of subsequent DTG maxima representing the portions of OH groups that did not dehydroxylate in previous cycles. Each stage of partial dehydroxylation consists of two kinetic mechanisms and for each of them the experimental dα/dt values that characterize the reaction rate of the dehydroxylated fraction, α, within a period of the reaction time, t, were computed. One mechanism corresponds to a zero-order reaction that occurs in each cycle and indicates that the reaction is homogeneous and each non-dehydoxylated layer is transformed into metakaolinite layer without formation of intermediate derivatives. For this step of the cycles activation energy, Ea, was calculated from the linear relationship between ln(dα/dt) and reciprocal temperature, T; for KGa-2 kaolinite, the Ea varies from 32.0 to 38.1 kcal/mol; in KGa-1, Ea varies from 37.1 to 40.4 kcal/mol, whereas in Keokuk, Ea varies from 42.7 to 47.5 kcal/mol. The particular variation of the Ea is discussed in terms of structural and morphological features of the samples. where n is an empirical parameter and its value was found from n controls the reaction rate slowing or the deviation from the zero-order reaction and increases with increasing metakaolinite content. Using parameters n, α, and T determined for the second step, Ea values were calculated for the second step of reaction in each heating cycle. For the Keokuk kaolinite, Ea value varies from 31.6 to 37.5 kcal/mol, in KGa-1 Ea is 27.0–35.6 kcal/mol, and in KGa-2 the Ea value varies from 26.3 to 34.9 kcal/mol. A structural model explaining the acceleration rate slowing is discussed.Keywords
This publication has 29 references indexed in Scilit:
- Mechanism of dehydroxylation temperature decrease and high temperature phase transition of coal-bearing strata kaolinite intercalated by potassium acetateJournal of Colloid and Interface Science, 2012
- Nature of rehydroxylation in dioctahedral 2:1 layer clay mineralsAmerican Mineralogist: Journal of Earth and Planetary Materials, 2012
- Dehydroxylation and Rehydroxylation Mechanisms in Fired Clay Ceramic: A TG‐MS and DRIFTS InvestigationJournal of the American Ceramic Society, 2011
- XRD study of the dehydration and rehydration behaviour of Al-pillared smectites differing in source of chargeJournal of Thermal Analysis and Calorimetry, 1997
- Rietveld Refinement of the Kaolinite Structure at 1.5 KClays and Clay Minerals, 1993
- Rietveld Refinement of Non-Hydrogen Atomic Positions in KaoliniteClays and Clay Minerals, 1989
- Stacking Faults in Kaolin-Group Minerals in the Light of Real Structural FeaturesClays and Clay Minerals, 1989
- Chapter 2. POLYTYPISM OF 1:1 LAYER SILICATES1988
- Kinetics of Dehydroxylation of Kaolinite and HalloysiteJournal of the American Ceramic Society, 1957
- The structure of kaoliniteMineralogical Magazine and Journal of the Mineralogical Society, 1946