Microstructure Transformation Behavior of Hot‐Rolled Steel Oxide Scale during the Preheating Process
Authors:
- 15 December 2020
- journal article
- research article
- Published by Wiley in Steel Research International
- Vol. 92 (5)
Abstract
The microstructure transformation of oxide scale in hot‐rolled steel strips during the preheating process is studied by thermal simulation at temperatures ranging from 530 to 800 °C. The results show that the original structure of the oxide scale comprises an outer Fe3O4 layer, an inner Fe3O4/Fe eutectoid, and some precipitated Fe3O4. The Fe3O4/Fe eutectoid structure is first transformed into wüstite. After the eutectoid structure is completely transformed into wüstite, Fe3O4 precipitates are transformed into wüstite with aging. Then, white Fe is dissolved and diffused into wüstite to give a homogenous wüstite layer. The thickness of outer Fe3O4 layer decreases as the temperature increases, indicating that the outer Fe3O4 also transforms into wüstite. The heating rate and temperature are important parameters influencing the phase transformation of the oxide scale. More wüstite is formed at a slower heating rate and higher temperature; a larger number of pores are found inside the wüstite layer with increasing temperature; pores caused by transformation of the oxide scale are created by the density difference between wüstite and Fe3O4.Keywords
Funding Information
- National Natural Science Foundation of China (51301111)
- Natural Science Foundation of Liaoning Province (2019-KF-05-04)
This publication has 18 references indexed in Scilit:
- Corrosion kinetics and patina evolution of galvanized steel in a simulated coastal-industrial atmosphereJournal of Materials Science & Technology, 2019
- Effect of strip entry temperature on the formation of interfacial layer during hot-dip galvanizing of press-hardened steelSurface and Coatings Technology, 2014
- Selective Oxidation and Sub‐Surface Phase Transformation of TWIP Steel during Continuous AnnealingSteel Research International, 2011
- Effects of dew point on selective oxidation of TRIP steels containing Si, Mn, and BMetals and Materials International, 2011
- Internal Oxidation during Intercritical Annealing of CMnSi TRIP SteelISIJ International, 2009
- Formation of Surface and Subsurface Oxides during Ferritic, Intercritical and Austenitic Annealing of CMnSi TRIP SteelISIJ International, 2008
- Review of the High-Temperature Oxidation of Iron and Carbon Steels in Air or OxygenOxidation of Metals, 2003
- Galvanizability of high-strength steels for automotive applicationsMetallurgical and Materials Transactions A, 2001
- Oxide-Scale Structures Formed on Commercial Hot-Rolled Steel Strip and Their Formation MechanismsOxidation of Metals, 2001
- A Study of the Scale Structure of Hot-Rolled Steel Strip by Simulated Coiling and CoolingOxidation of Metals, 2000