Abstract
The H1 NMR average effective spin-lattice relaxation rate 1∕T1 has been measured as a function of magnetic field (4.5–15.6T) at T=1 and 0.3K, and as a function of temperature (0.07–1K) around the first crossing field Hc1=7.43T, in the molecular antiferromagnetic ring [Cr8F8Piv16] (Cr8). T1−1(H) shows a single peak centered at Hc1 and a double peak for H≃Hc2. The field dependence of 1∕T1 away from the level crossing can be explained by a nuclear relaxation mechanism due to quasielastic scattering in the S=1 excited state thus yielding the energy gap between S=0 and S=1, MS=−1 states. An additional contribution to T1−1 can be detected near Hc1, due to inelastic scattering. Information about the H and T dependence of the width of the molecular magnetic levels is obtained from the fit of the T1−1 data.

This publication has 20 references indexed in Scilit: