Effect of Contact Plug Deposition Conditions on Junction Leakage and Contact Resistance in Multilevel CMOS Logic Interconnection Device
Open Access
- 6 February 2020
- journal article
- research article
- Published by MDPI AG in Micromachines
- Vol. 11 (2) , 170
Abstract
Here, we developed the optimal conditions in terms of physical and electrical characteristics of the barrier and tungsten (W) deposition process of a contact module, which is the segment connecting the device and the multi-layer metallization (MLM) metal line in the development of 100 nm-class logic devices. To confirm its applicability to the logic contact of barrier and W films, a contact hole was formed, first to check the bottom coverage and the filling status of each film, then to check the electrical resistance and leakage characteristics to analyze the optimal conditions. At an aspect ratio of 3.89:1, ionized metal plasma (IMP) Ti had a bottom coverage of 40.9% and chemical vapor deposition (CVD) titanium nitride (TiN) of 76.2%, confirming that it was possible to apply the process to 100 nm logic contacts. W filling was confirmed, and a salicide etching rate (using Radio Frequency (RF) etch) of 13–18 Å/s at a 3.53:1 aspect ratio was applied. The etching rate on the thermal oxide plate was 9 Å/s. As the RF etch amount increased from 50–100 Å, the P active resistance increased by 0.5–1 Ω. The resistance also increased as the amount of IMP Ti deposition increased to 300 Å. A measurement of the borderless contact junction leakage current indicated that the current in the P + N well increased by more than an order of magnitude when IMP Ti 250 Å or more was deposited. The contact resistance value was 0.5 Ω. An AC bias improved the IMP Ti deposition rate by 10% in bottom coverage, but there was no significant difference in contact resistance. In the case of applying IMP TiN, the overall contact resistance decreased to 2 Ω compared to CVD TiN, but the distribution characteristics were poor. The best results were obtained under the conditions of RF etch 50 Å, IMP Ti 200 Å, and CVD TiN 2 × 50 Å.Keywords
This publication has 36 references indexed in Scilit:
- Investigation of the layout and optical proximity correction effects to control the trench etching process on 4H-SiCElectronic Materials Letters, 2017
- Experimental Study on Reaction Characteristics of PTFE/Ti/W Energetic Materials under Explosive LoadingMaterials, 2016
- Electroless and Electrolytic Copper Plating of Glass Interposer Combined with Metal Oxide Adhesion Layer for Manufacturing 3D RF Devices2016
- Seed Growth of Tungsten Diselenide Nanotubes from Tungsten OxidesSmall, 2015
- Transistor scaling with novel materialsMaterials Today, 2006
- Etch Defect Reduction Using SF6/O2 Plasma Cleaning and Optimizing Etching Recipe in Photo Resist Masked Gate Poly Silicon Etch ProcessJapanese Journal of Applied Physics, 2005
- The impact of etch-stop layer for borderless contacts on deep submicron CMOS device performance—a comparative studyThin Solid Films, 2004
- Formation of low resistance Pt ohmic contacts to p-type GaN using two-step surface treatmentJournal of Vacuum Science & Technology B: Microelectronics and Nanometer Structures Processing, Measurement, and Phenomena, 1999
- High aspect ratio contacts: A review of the current tungsten plug processThin Solid Films, 1997
- An XPS study of the adherence of refractory carbide silicide and boride rf-sputtered wear-resistant coatingsJournal of Vacuum Science and Technology, 1978